General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 3 % Show Supplier Material materials with Elongación of 3 % | SABIC - Japan Method | break |
Impact strength, Izod notched, ASTM | 23.0 °C | 88 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 88 J/m | ASTM D 256 |
Módulo de flexión | 23.0 °C | 12.1 GPa Show Supplier Material materials with Módulo de flexión of 12.1 GPa | ASTM D 790 |
Resistencia a la flexión | 23.0 °C | 216 MPa Show Supplier Material materials with Resistencia a la flexión of 216 MPa | ASTM D 790 |
Resistencia a la tracción | 23.0 °C | 154 MPa Show Supplier Material materials with Resistencia a la tracción of 154 MPa | SABIC - Japan Method | yield |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 88 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 88 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 6E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6E-5 1/K | TMA | -30°C to 30°C | ||
Heat deflection temperature, 0.45 MPa | 206 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 206 °C | ASTM D 648 | 3.2 mm, unannealed | |||
Relative temperature index, electrical | 75 °C Show Supplier Material materials with Relative temperature index, electrical of 75 °C | UL 746B | |||
Relative temperature index, mechanical impact | 75 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 75 °C | UL 746B | |||
Relative temperature index, mechanical strength | 75 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 75 °C | UL 746B | |||
Temperatura de flexión bajo carga | 206 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 206 °C | ||||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=236842- - <br> UL Recognized, 94V-0 Flame Class Rating: 1.5mm UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 1.00E+3 - 1.00E+8 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+3 - 1.00E+8 Ω | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.1 % Show Supplier Material materials with Contracción of 0.1 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Document Handling | |
Availability | Europe,Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |