General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 3 % Show Supplier Material materials with Elongación of 3 % | SABIC - Japan Method | break |
Impact strength, Izod notched, ASTM | 23.0 °C | 76 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 76 J/m | ASTM D 256 |
Módulo de flexión | 23.0 °C | 17.5 GPa Show Supplier Material materials with Módulo de flexión of 17.5 GPa | ASTM D 790 |
Resistencia a la flexión | 23.0 °C | 238 MPa Show Supplier Material materials with Resistencia a la flexión of 238 MPa | ASTM D 790 |
Resistencia a la tracción | 23.0 °C | 166 MPa Show Supplier Material materials with Resistencia a la tracción of 166 MPa | SABIC - Japan Method | yield |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 76 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 76 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 5E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 5E-5 1/K | TMA | -30°C to 30°C | ||
Heat deflection temperature, 0.45 MPa | 205 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 205 °C | ASTM D 648 | 3.2 mm, unannealed | |||
Relative temperature index, electrical | 75 °C Show Supplier Material materials with Relative temperature index, electrical of 75 °C | UL 746B | |||
Relative temperature index, mechanical impact | 75 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 75 °C | UL 746B | |||
Relative temperature index, mechanical strength | 75 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 75 °C | UL 746B | |||
Temperatura de flexión bajo carga | 205 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 205 °C | ||||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=236843- - <br> UL Recognized, 94V-0 Flame Class Rating: 1.5mm UL 94 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.1 % Show Supplier Material materials with Contracción of 0.1 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Toy | |
Availability | Europe,Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |