General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.35 % Show Supplier Material materials with Absorción de agua of 0.35 % | ASTM D 570 | (23°C/Saturated) |
Densidad | 23.0 °C | 1.19 g/cm³ Show Supplier Material materials with Densidad of 1.19 g/cm³ | ASTM D 792 |
Densidad relativa | 23.0 °C | 1.2 [-] Show Supplier Material materials with Densidad relativa of 1.2 [-] | ASTM D 792 | |
Specific volume | 23.0 °C | 0.83 cm³/g Show Supplier Material materials with Specific volume of 0.83 cm³/g | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Rockwell M | 23.0 °C | 70 [-] Show Supplier Material materials with Dureza Rockwell M of 70 [-] | ASTM D 785 | |
Elongación | 23.0 °C | 110 % Show Supplier Material materials with Elongación of 110 % | ASTM D 638 | brk, Type I, 50 mm/min |
Hardness, Rockwell R | 23.0 °C | 118 [-] Show Supplier Material materials with Hardness, Rockwell R of 118 [-] | ASTM D 785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 907 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 907 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 3204 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 3204 J/m | ASTM D 4812 | 23°C |
Módulo de flexión | 23.0 °C | 2.3 GPa Show Supplier Material materials with Módulo de flexión of 2.3 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Resistencia a la flexión | 23.0 °C | 93 MPa Show Supplier Material materials with Resistencia a la flexión of 93 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Resistencia a la tracción | 23.0 °C | 65 MPa Show Supplier Material materials with Resistencia a la tracción of 65 MPa | ASTM D 638 | brk, Type I, 50 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 907 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 907 kJ/m² | ASTM D 256 | notched, 23°C |
Taber Abrasion | 23.0 °C | 10 mg/1000cy Show Supplier Material materials with Taber Abrasion of 10 mg/1000cy | ASTM D 1044 | CS-17, 1 kg |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Calor específico | 23.0 °C | 1.26E-3 J/(kg·K) Show Supplier Material materials with Calor específico of 1.26E-3 J/(kg·K) | ASTM C 351 | ||
Coeficiente de dilatación térmica | 23.0 °C | 6.84E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6.84E-5 1/K | ASTM E 831 | -40°C to 95°C | ||
Conductividad térmica | 23.0 °C | 0.29 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.29 W/(m·K) | ASTM C177 | ||
Heat deflection temperature, 0.45 MPa | 137 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 137 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 132 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 132 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |||
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | UL 746B | |||
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | UL 746B | |||
Temperatura de flexión bajo carga | 132 - 137 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 132 - 137 °C | ||||
Temperatura de reblandecimiento Vicat | 154 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 154 °C | ASTM D 1525 | Rate B/50 | |||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=103952989- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥6mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.75mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.75mm UL 94 <br> UV-light, water exposure/immersion: F1- UL 746C |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 23.0 °C | 2.96 [-] Show Supplier Material materials with Constante dieléctrica, 1 MHz of 2.96 [-] | ASTM D 150 |
Dielectric constant, 60Hz | 23.0 °C | 3.17 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 3.17 [-] | ASTM D 150 | 50/60 Hz |
Dissipation factor, 1MHz | 23.0 °C | 0.01 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 0.01 [-] | ASTM D 150 | |
Dissipation factor, 50Hz | 23.0 °C | 9E-4 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 9E-4 [-] | ASTM D 150 | 50/60 Hz |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 2 |
High Volt Arc Track Rate | 23.0 °C | 2 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 2 |
Rigidez dieléctrica | 23.0 °C | 15 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 15 kV/mm | ASTM D 149 | in air, 3.2 mm |
Volume resistivity | 23.0 °C | 1.00E+17 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+17 Ω·cm | ASTM D 257 |
Índice de seguimiento comparativo | 23.0 °C | 2 V Show Supplier Material materials with Índice de seguimiento comparativo of 2 V | UL 746A | (UL) {PLC} |
Óptico
Property | Value | Comment |
---|---|---|
Transmission | 88 % Show Supplier Material materials with Transmission of 88 % | ASTM D 1003 | 2.54 mm |
Turbidez | 1 % Show Supplier Material materials with Turbidez of 1 % | ASTM D 1003 | 2.54 mm |
Índice de refracción | 1.59 [-] Show Supplier Material materials with Índice de refracción of 1.59 [-] | ASTM D542 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |