General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 3 - 4 % Show Supplier Material materials with Elongación of 3 - 4 % | ASTM D 638 | brk, Type I, 5 mm/min |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1010 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1010 J/m | ASTM D 4812 | 23°C |
Módulo de flexión | 23.0 °C | 8.3 GPa Show Supplier Material materials with Módulo de flexión of 8.3 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Resistencia a la flexión | 23.0 °C | 227 MPa Show Supplier Material materials with Resistencia a la flexión of 227 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Resistencia a la tracción | 23.0 °C | 158 MPa Show Supplier Material materials with Resistencia a la tracción of 158 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 187 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 187 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.4 % Show Supplier Material materials with Contracción of 0.4 % | SABIC method |
Technological properties
Property | ||
---|---|---|
Application areas | Oil/Gas, Electronic Components | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |