General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.66 g/cm³ Show Supplier Material materials with Densidad of 1.66 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Impact strength, Izod notched, ASTM | 23.0 °C | 60 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 60 J/m | ASTM D 256 | notched, 23°C |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 60 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 60 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 0.45 MPa | 134 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 134 °C | ASTM D 648 | 3.2 mm, unannealed |
Heat deflection temperature, 1.80 MPa | 122 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 122 °C | ASTM D 648 | 3.2mm, unannealed |
Temperatura de flexión bajo carga | 122 - 134 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 122 - 134 °C |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 1GHz | 23.0 °C | 4.4 [-] Show Supplier Material materials with Dielectric constant, 1GHz of 4.4 [-] | ASTM ES 7-83 | 1.1 GHz |
Dissipation factor, 1GHz | 23.0 °C | 2E-3 [-] Show Supplier Material materials with Dissipation factor, 1GHz of 2E-3 [-] | ASTM ES 7-83 | 1.1 GHz |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.7 % Show Supplier Material materials with Contracción of 0.7 % | ASTM D 955 | 24 hrs |
Contracción transversal | 23.0 °C | 0.65 % Show Supplier Material materials with Contracción transversal of 0.65 % | ASTM D 955 | 24 hrs |
Velocidad de flujo del volumen derretido | 11 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 11 cm³/10min | ISO 1133 | MVR at 300°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Wireless Communications, Wiring Devices, Cooking Range | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 105°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |