General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad relativa | 23.0 °C | 1.24 [-] Show Supplier Material materials with Densidad relativa of 1.24 [-] | ASTM D 792 | |
Moisture absorption | 23.0 °C | 0.3 % Show Supplier Material materials with Moisture absorption of 0.3 % | ASTM D 570 | (23°C/50% RH/24 hrs) |
Índice límite de óxigeno | 23.0 °C | 26 % Show Supplier Material materials with Índice límite de óxigeno of 26 % |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 5.6E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 5.6E-5 1/K | ASTM D 696 | -30°C to 30°C |
Heat deflection temperature, 1.80 MPa | 174 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 174 °C | ASTM D 648 | 3.2mm, unannealed | |
Temperatura de flexión bajo carga | 174 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 174 °C |
Eléctrico
Technological properties
Property | ||
---|---|---|
Application areas | Monitoring and Imaging, Medical Device | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120 to 150.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |