General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 4.5 % Show Supplier Material materials with Elongación of 4.5 % | ISO 527 | yield, 5 mm/min |
Módulo elástico | 23.0 °C | 2.4 GPa Show Supplier Material materials with Módulo elástico of 2.4 GPa | ISO 527 | 1 mm/min |
Resistencia a la tracción | 23.0 °C | 62 MPa Show Supplier Material materials with Resistencia a la tracción of 62 MPa | ISO 527 | yield, 5 mm/min |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 0.45 MPa | 135 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 135 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm |
Heat deflection temperature, 1.80 MPa | 62 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 62 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm |
Temperatura de flexión bajo carga | 62 - 135 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 62 - 135 °C |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 23.0 °C | 3.2 [-] Show Supplier Material materials with Constante dieléctrica, 1 MHz of 3.2 [-] | ASTM D 150 |
Constante dieléctrica, 100 Hz | 23.0 °C | 3.6 [-] Show Supplier Material materials with Constante dieléctrica, 100 Hz of 3.6 [-] | ASTM D 150 |
Dissipation factor, 100Hz | 23.0 °C | 0.02 [-] Show Supplier Material materials with Dissipation factor, 100Hz of 0.02 [-] | ASTM D 150 |
Dissipation factor, 100kHz | 23.0 °C | 0.01 [-] Show Supplier Material materials with Dissipation factor, 100kHz of 0.01 [-] | ASTM D 150 |
Dissipation factor, 1kHz | 23.0 °C | 0.02 [-] Show Supplier Material materials with Dissipation factor, 1kHz of 0.02 [-] | ASTM D 150 |
Sheet resistivity, ROA | 23.0 °C | 1.00E+12 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+12 Ω | ASTM D 257 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |