General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 1.25 % Show Supplier Material materials with Absorción de agua of 1.25 % | ISO 62-1 | (23°C/saturated) |
Densidad | 23.0 °C | 1.27 g/cm³ Show Supplier Material materials with Densidad of 1.27 g/cm³ | ISO 1183 |
Densidad relativa | 23.0 °C | 1.27 [-] Show Supplier Material materials with Densidad relativa of 1.27 [-] | ASTM D 792 | |
Moisture absorption | 23.0 °C | 0.7 % Show Supplier Material materials with Moisture absorption of 0.7 % | ISO 62 | (23°C / 50% RH) |
Índice límite de óxigeno | 23.0 °C | 47 % Show Supplier Material materials with Índice límite de óxigeno of 47 % |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.3 [-] | ASTM E 132 | ||
Elongación | 23.0 °C | 6 % Show Supplier Material materials with Elongación of 6 % | ISO 527 | yield, 50 mm/min | ||
Hardness, Ball Indentation | 23.0 °C | 140 MPa Show Supplier Material materials with Hardness, Ball Indentation of 140 MPa | ISO 2039-1 | H358/30 | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 53 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 53 J/m | ASTM D 256 | ||
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1335 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1335 J/m | ASTM D 4812 | 23°C | ||
Instrumented Impact, Total Energy | 23.0 °C | 38 J Show Supplier Material materials with Instrumented Impact, Total Energy of 38 J | ASTM D 3763 | 23°C | ||
Módulo de flexión | 23.0 °C | 3.3 GPa Show Supplier Material materials with Módulo de flexión of 3.3 GPa | ISO 178 | 2 mm/min | ||
Módulo elástico | 23.0 °C | 3.2 GPa Show Supplier Material materials with Módulo elástico of 3.2 GPa | ISO 527 | 1 mm/min | ||
Resistencia a la flexión | 23.0 °C | 160 MPa Show Supplier Material materials with Resistencia a la flexión of 160 MPa | ISO 178 | yield, 2 mm/min | ||
Resistencia a la tracción | 23.0 °C | 105 MPa Show Supplier Material materials with Resistencia a la tracción of 105 MPa | ISO 527 | yield, 50 mm/min | ||
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | ISO 179/2C | 23°C | ||
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 6 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C | ||
Taber Abrasion | 23.0 °C | 10 mg/1000cy Show Supplier Material materials with Taber Abrasion of 10 mg/1000cy | SABIC method | CS-17, 1 kg | ||
Resistencia al choque, ensayo Izod no entallado | ISO 180/1U | unnotched 80*10*4, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | 125°C +/- 2°C | |||
Coeficiente de dilatación térmica | 23.0 °C | 5E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 5E-5 1/K | ISO 11359-2 | 23°C to 150°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 5E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 5E-5 1/K | ISO 11359-2 | 23°C to 150°C | ||
Conductividad térmica | 23.0 °C | 0.24 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.24 W/(m·K) | ISO 8302 | ||
Heat deflection temperature, 0.45 MPa | 200 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 200 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 190 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 190 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Temperatura de flexión bajo carga | 190 - 200 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 190 - 200 °C | ||||
Temperatura de reblandecimiento Vicat | 211 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 211 °C | ISO 306 | Rate B/50 | |||
Inflamabilidad | Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 23.0 °C | 2.9 [-] Show Supplier Material materials with Constante dieléctrica, 1 MHz of 2.9 [-] | IEC 60250 |
Constante dieléctrica, 100 Hz | 23.0 °C | 3.15 [-] Show Supplier Material materials with Constante dieléctrica, 100 Hz of 3.15 [-] | ASTM D 150 |
Dielectric constant, 60Hz | 23.0 °C | 2.9 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.9 [-] | IEC 60250 | 50/60 Hz |
Dissipation factor, 100Hz | 23.0 °C | 1.5E-3 [-] Show Supplier Material materials with Dissipation factor, 100Hz of 1.5E-3 [-] | ASTM D 150 |
Dissipation factor, 1MHz | 23.0 °C | 6E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 6E-3 [-] | IEC 60250 |
Dissipation factor, 1kHz | 23.0 °C | 1.2E-3 [-] Show Supplier Material materials with Dissipation factor, 1kHz of 1.2E-3 [-] | ASTM D 150 |
Dissipation factor, 50Hz | 23.0 °C | 5E-4 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 5E-4 [-] | IEC 60250 | 50/60 Hz |
Factor de disipación | 23.0 °C | 2.5E-3 [-] Show Supplier Material materials with Factor de disipación of 2.5E-3 [-] | IEC 60250 | 2450 MHz |
Rigidez dieléctrica | 23.0 °C | 16 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 16 kV/mm | IEC 60243-1 | in oil, 3.2 mm, |
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | >, IEC 60093 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | IEC 60093 |
Índice de seguimiento comparativo | 23.0 °C | 150 V Show Supplier Material materials with Índice de seguimiento comparativo of 150 V | IEC 60112 | |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 9 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 9 g/10min | ASTM D 1238 | 337°C/6.6 kgf | |
Velocidad de flujo del volumen derretido | 13 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 13 cm³/10min | ISO 1133 | MVR at 360°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Surgical Devices, Commercial Storage/Cookware, Airline Service, Food Container, Food Processor, Food Transportation | |
Availability | Europe,Asia,Americas | |
Processing methods | Middle - Zone 2 Temperature: 340 to 400.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |