General
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.39 - 0.44 [-] Show Supplier Material materials with Coefficient of friction of 0.39 - 0.44 [-] | ||
Coefficient of friction, kinetic | 0.39 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.39 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.44 [-] Show Supplier Material materials with Coefficient of friction, static of 0.44 [-] | ASTM D 3702 Modified: Manual | |
Densidad | 23.0 °C | 1.14 g/cm³ Show Supplier Material materials with Densidad of 1.14 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.2 % Show Supplier Material materials with Moisture absorption of 0.2 % | ASTM D 570 | (23°C/50% RH/24 hrs) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 28 % Show Supplier Material materials with Elongación of 28 % | ISO 527 | break |
Impact strength, Izod notched, ASTM | 23.0 °C | 80 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 80 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 560 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 560 J/m | ASTM D 4812 | 23°C |
Módulo de flexión | 23.0 °C | 2.3 GPa Show Supplier Material materials with Módulo de flexión of 2.3 GPa | ISO 178 |
Módulo elástico | 23.0 °C | 2.3 GPa Show Supplier Material materials with Módulo elástico of 2.3 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 59 MPa Show Supplier Material materials with Resistencia a la flexión of 59 MPa | ISO 178 |
Resistencia a la tracción | 23.0 °C | 31 MPa Show Supplier Material materials with Resistencia a la tracción of 31 MPa | ISO 527 | break |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 8 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 33 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 33 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Aplicaciones térmicas
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Lab Ware and Clinical Diagnostics, Tray | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |