General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 50 - 100 % Show Supplier Material materials with Elongación of 50 - 100 % | ASTM D 638 | brk, Type I, 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 69 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 69 J/m | ASTM D 256 |
Módulo de flexión | 23.0 °C | 2.7 GPa Show Supplier Material materials with Módulo de flexión of 2.7 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Módulo elástico | 23.0 °C | 2.5 GPa Show Supplier Material materials with Módulo elástico of 2.5 GPa | ASTM D 638 | 50 mm/min |
Resistencia a la flexión | 23.0 °C | 106 MPa Show Supplier Material materials with Resistencia a la flexión of 106 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Resistencia a la tracción | 23.0 °C | 70.3 MPa Show Supplier Material materials with Resistencia a la tracción of 70.3 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 69 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 69 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 5.6E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 5.6E-5 1/K | ASTM D 696 | -30°C to 30°C |
Heat deflection temperature, 1.80 MPa | 174 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 174 °C | ASTM D 648 | 3.2mm, unannealed | |
Temperatura de flexión bajo carga | 174 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 174 °C |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Dissipation factor, 1MHz | 23.0 °C | 3.02 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 3.02 [-] | ASTM D 150 | |
Dissipation factor, 1kHz | 23.0 °C | 3.04 [-] Show Supplier Material materials with Dissipation factor, 1kHz of 3.04 [-] | ASTM D 150 |
Dissipation factor, 50Hz | 23.0 °C | 3.03 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 3.03 [-] | ASTM D 150 | 50/60 Hz |
Volume resistivity | 23.0 °C | 5.00E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 5.00E+16 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.7 % Show Supplier Material materials with Contracción of 0.7 % | ASTM D 955 | 24 hrs |
Velocidad de flujo de la masa derretida | 17 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 17 g/10min | ASTM D 1238 | 330°C/2.16 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Others, Surgical Tray, Surgical Devices | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 135 to 163.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |