General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.38 g/cm³ Show Supplier Material materials with Densidad of 1.38 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Impact strength, Izod notched, ASTM | 23.0 °C | 86 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 86 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 410 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 410 J/m | ASTM D 4812 | 23°C |
Módulo de flexión | 23.0 °C | 12.5 GPa Show Supplier Material materials with Módulo de flexión of 12.5 GPa | ASTM D 790 |
Módulo elástico | 23.0 °C | 14 GPa Show Supplier Material materials with Módulo elástico of 14 GPa | ASTM D 638 | 50 mm/min |
Resistencia a la flexión | 23.0 °C | 214 MPa Show Supplier Material materials with Resistencia a la flexión of 214 MPa | ASTM D 790 |
Resistencia a la tracción | 23.0 °C | 152 MPa Show Supplier Material materials with Resistencia a la tracción of 152 MPa | ASTM D 638 | brk, Type I, 50 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 86 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 86 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 0.45 MPa | 143 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 143 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm |
Heat deflection temperature, 1.80 MPa | 137 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 137 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm |
Temperatura de flexión bajo carga | 137 - 143 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 137 - 143 °C |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100 - 10000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100 - 10000 Ω | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Application areas | Medical Device, Document Handling, Enclosures | |
Availability | Europe,Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |