General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.96 g/cm³ Show Supplier Material materials with Densidad of 0.96 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 4.1 % Show Supplier Material materials with Elongación of 4.1 % | ISO 527 | break, 5 mm/min |
Módulo de flexión | 23.0 °C | 2.3 GPa Show Supplier Material materials with Módulo de flexión of 2.3 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 3 GPa Show Supplier Material materials with Módulo elástico of 3 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 74 MPa Show Supplier Material materials with Resistencia a la flexión of 74 MPa | ISO 178 | yield, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 44 MPa Show Supplier Material materials with Resistencia a la tracción of 44 MPa | ISO 527 | break, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 8 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 29 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 29 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 6.6E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6.6E-5 1/K | ASTM D 696 | -30°C to 30°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 8.8E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 8.8E-5 1/K | ASTM D 696 | -30°C to 30°C | ||
Glow Wire Flammability Index | 850 °C Show Supplier Material materials with Glow Wire Flammability Index of 850 °C | ||||
Glow Wire Ignition Temperature | 875 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 875 °C | IEC 60695-2-13 | 3.0 mm | |||
Heat deflection temperature, 0.45 MPa | 146 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 146 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 99 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 99 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | UL 746B | |||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | UL 746B | |||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | UL 746B | |||
Temperatura de flexión bajo carga | 99 - 146 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 99 - 146 °C | ||||
Inflamabilidad | UL Recognized, 94HB Flame Class Rating: ≥1mm UL 94 <br> Glow Wire Ignitability Temperature, 1.5 mm: 850°C IEC 60695-2-13 <br> Glow Wire Flammability Index, 1.5 mm: 850°C IEC 60695-2-12 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=103716364- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 1 mm Show Supplier Material materials with High Amp Arc Ignition of 1 mm | ≥, UL 746A | PLC 3 |
High Volt Arc Track Rate | 23.0 °C | 1 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 1 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1 mm Show Supplier Material materials with Hot-Wire Ignition of 1 mm | ≥, UL 746A | PLC 3 |
Índice de seguimiento comparativo | 23.0 °C | 0 V Show Supplier Material materials with Índice de seguimiento comparativo of 0 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 1 % Show Supplier Material materials with Contracción of 1 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Non-LED Lighting | |
Availability | Europe,Americas | |
Processing methods | Middle - Zone 2 Temperature: 215 to 225.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |