General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore A | 23.0 °C | 79 [-] Show Supplier Material materials with Dureza Shore A of 79 [-] | ASTM D 2240 | 30S reading |
Elongación | 23.0 °C | 215 % Show Supplier Material materials with Elongación of 215 % | ISO 527 | break, 50 mm/min |
Módulo de flexión | 23.0 °C | 0 GPa Show Supplier Material materials with Módulo de flexión of 0 GPa | ISO 178 | 12.5 mm/min |
Resistencia a la tracción | 23.0 °C | 14 MPa Show Supplier Material materials with Resistencia a la tracción of 14 MPa | ISO 527 | break, 50 mm/min |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Brittleness temperature | -40 °C Show Supplier Material materials with Brittleness temperature of -40 °C | <, ASTM D 746 | |
Glow Wire Ignition Temperature | 800 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 800 °C | IEC 60695-2-13 | 3.0 mm | |
Inflamabilidad | Smoke Density on 0.5mm plaque, Flame, Ds, max: 117- ASTM E 662 <br> Smoke Density on 0.5mm plaque, Non-flame, Ds, max: 70- ASTM E 662 <br> Glow Wire Flammability Index 960°C, passes at: 3mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 3mm IEC 60695-2-12 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 23.0 °C | 2.6 [-] Show Supplier Material materials with Constante dieléctrica, 1 MHz of 2.6 [-] | ASTM D 150 |
Dissipation factor, 1MHz | 23.0 °C | 7E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 7E-3 [-] | ASTM D 150 |
Rigidez dieléctrica | 23.0 °C | 24.5 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 24.5 kV/mm | IEC 60243-1 | in oil, 2.0mm |
Volume resistivity | 23.0 °C | 1.40E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 1.40E+16 Ω·cm | ASTM D 257 |
Índice de seguimiento comparativo | 23.0 °C | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | IEC 60112 | |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 11 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 11 g/10min | ASTM D 1238 | 250°C/10.0 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Wiring Devices, Personal Computing, Wire & cable | |
Availability | Asia,Americas | |
Processing methods | Die Temperature: 220 to 250.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |