General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.19 g/cm³ Show Supplier Material materials with Densidad of 1.19 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 7 % Show Supplier Material materials with Elongación of 7 % | ISO 527 | brk, Type I, 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 170 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 170 J/m | ASTM D 256 | notched, -30°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1000 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1000 J/m | ASTM D 256 | un-notched, -30°C |
Instrumented Impact, Total Energy | 23.0 °C | 10 J Show Supplier Material materials with Instrumented Impact, Total Energy of 10 J | ASTM D 3763 | -30 °C |
Módulo de flexión | 23.0 °C | 2 GPa Show Supplier Material materials with Módulo de flexión of 2 GPa | ISO 178 | 1.3 mm/min |
Módulo elástico | 23.0 °C | 1.8 GPa Show Supplier Material materials with Módulo elástico of 1.8 GPa | ISO 527 | brk, Type I, 5 mm/min |
Resistencia a la tracción | 23.0 °C | 49 MPa Show Supplier Material materials with Resistencia a la tracción of 49 MPa | ISO 527 | brk, Type I, 5 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | ISO 179 | notched, 23°C |
Resistencia al choque, ensayo Charpy no entallado | 23.0 °C | 88 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 88 kJ/m² | ISO 179 | un-notched, 23°C |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 18 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 18 kJ/m² | ISO 180 | notched, 23°C, |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 22 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 22 kJ/m² | ISO 180 | un-notched, -30°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 7.7E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7.7E-5 1/K | ASTM E 831 | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 77 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 77 1/K | ASTM E 831 | ||
Heat deflection temperature, 1.80 MPa | 137 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 137 °C | ISO 75 | 3.2 mm, unannealed | |||
Temperatura de flexión bajo carga | 137 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 137 °C | ||||
Temperatura de reblandecimiento Vicat | 149 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 149 °C | ISO 306 | Rate A/50 | |||
Inflamabilidad | UL94 Flame Class Rating: V-0- UL 94 <br> UL94 Flame Class Rating: V-0- UL 94 <br> UL94 Flame Class Rating: V-2- UL 94 <br> UL94 Flame Class Rating: V-2- UL 94 <br> UL94 Flame Class Rating: V-2- UL 94 <br> UL94 Flame Class Rating: V-2- UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica | 23.0 °C | 2.6 [-] Show Supplier Material materials with Constante dieléctrica of 2.6 [-] | ASTM D150 |
Factor de disipación | 23.0 °C | 5E-3 [-] Show Supplier Material materials with Factor de disipación of 5E-3 [-] | ASTM D 150 | |
Volume resistivity | 23.0 °C | 1.50E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.50E+15 Ω·cm | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Application areas | Additive Plastic | |
Availability | Europe,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |