General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad relativa | 23.0 °C | 1.39 [-] Show Supplier Material materials with Densidad relativa of 1.39 [-] | ASTM D 792 | |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 3 % Show Supplier Material materials with Elongación of 3 % | ASTM D 638 | yld, Type I, 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 80 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 80 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 587 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 587 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 14 J Show Supplier Material materials with Instrumented Impact, Total Energy of 14 J | ASTM D 3763 | 23°C |
Módulo de flexión | 23.0 °C | 6.9 GPa Show Supplier Material materials with Módulo de flexión of 6.9 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Módulo elástico | 23.0 °C | 6.9 GPa Show Supplier Material materials with Módulo elástico of 6.9 GPa | ASTM D 638 | 5 mm/min |
Resistencia a la flexión | 23.0 °C | 206 MPa Show Supplier Material materials with Resistencia a la flexión of 206 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Resistencia a la tracción | 23.0 °C | 137 MPa Show Supplier Material materials with Resistencia a la tracción of 137 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 80 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 80 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 3.6E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3.6E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 7.2E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 7.2E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Heat deflection temperature, 0.45 MPa | 211 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 211 °C | ASTM D 648 | 3.2 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 206 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 206 °C | ASTM D 648 | 3.2mm, unannealed | |||
Relative temperature index, electrical | 105 °C Show Supplier Material materials with Relative temperature index, electrical of 105 °C | UL 746B | |||
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |||
Relative temperature index, mechanical strength | 105 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 105 °C | UL 746B | |||
Temperatura de flexión bajo carga | 206 - 211 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 206 - 211 °C | ||||
Temperatura de reblandecimiento Vicat | 210 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 210 °C | ASTM D 1525 | Rate B/50 | |||
Inflamabilidad | UL Recognized, 94V-0 Flame Class Rating: ≥0.4mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221095- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=221096- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 0.4 mm Show Supplier Material materials with High Amp Arc Ignition of 0.4 mm | ≥, UL 746A | PLC 4 |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 0.75 mm Show Supplier Material materials with Hot-Wire Ignition of 0.75 mm | ≥, UL 746A | PLC 3 |
Índice de seguimiento comparativo | 23.0 °C | 4 V Show Supplier Material materials with Índice de seguimiento comparativo of 4 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | SABIC method | 3.2 mm |
Contracción transversal | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción transversal of 0.5 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 13 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 13 g/10min | ASTM D 1238 | 337°C/6.6 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Enclosure/Housing/Cover, Circuit Protection, Semiconductor, Personal Computing, Wire & cable | |
Availability | Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |