General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad relativa | 23.0 °C | 1.06 [-] Show Supplier Material materials with Densidad relativa of 1.06 [-] | ASTM D 792 | |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 42 % Show Supplier Material materials with Elongación of 42 % | SABIC - Japan Method | break |
Impact strength, Izod notched, ASTM | 23.0 °C | 330 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 330 J/m | ASTM D 256 |
Módulo de flexión | 23.0 °C | 2.1 GPa Show Supplier Material materials with Módulo de flexión of 2.1 GPa | ASTM D 790 |
Resistencia a la flexión | 23.0 °C | 76 MPa Show Supplier Material materials with Resistencia a la flexión of 76 MPa | ASTM D 790 |
Resistencia a la tracción | 23.0 °C | 48 MPa Show Supplier Material materials with Resistencia a la tracción of 48 MPa | SABIC - Japan Method | yield |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 330 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 330 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 3.8 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 3.8 g/10min | ASTM D 1238 | 250°C/10.0 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Tray, Food Transportation, Industrial Material Handling | |
Availability | Asia | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |