General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad relativa | 23.0 °C | 1.27 [-] Show Supplier Material materials with Densidad relativa of 1.27 [-] | ASTM D 792 | |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Impact strength, Izod notched, ASTM | 23.0 °C | 16 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 16 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 470 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 470 J/m | ASTM D 4812 | 23°C |
Módulo de flexión | 23.0 °C | 3.5 GPa Show Supplier Material materials with Módulo de flexión of 3.5 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Módulo elástico | 23.0 °C | 3.3 GPa Show Supplier Material materials with Módulo elástico of 3.3 GPa | ASTM D 638 | 5 mm/min |
Resistencia a la flexión | 23.0 °C | 158 MPa Show Supplier Material materials with Resistencia a la flexión of 158 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Resistencia a la tracción | 23.0 °C | 96 MPa Show Supplier Material materials with Resistencia a la tracción of 96 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 16 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 16 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 6.7 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 6.7 g/10min | ASTM D 1238 | 295°C/6.6 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Enclosures | |
Availability | Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |