General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.2 % Show Supplier Material materials with Absorción de agua of 0.2 % | ISO 62-1 | (23°C/saturated) |
Densidad | 23.0 °C | 1.3 g/cm³ Show Supplier Material materials with Densidad of 1.3 g/cm³ | ISO 1183 |
Densidad relativa | 23.0 °C | 1.29 [-] Show Supplier Material materials with Densidad relativa of 1.29 [-] | ASTM D 792 | |
Moisture absorption | 23.0 °C | 0.06 % Show Supplier Material materials with Moisture absorption of 0.06 % | ISO 62 | (23°C / 50% RH) |
Índice límite de óxigeno | 23.0 °C | 26 % Show Supplier Material materials with Índice límite de óxigeno of 26 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2 % Show Supplier Material materials with Elongación of 2 % | ISO 527 | break, 5 mm/min |
Hardness, Ball Indentation | 23.0 °C | 130 MPa Show Supplier Material materials with Hardness, Ball Indentation of 130 MPa | ISO 2039-1 | H358/30 |
Módulo de flexión | 23.0 °C | 7.1 GPa Show Supplier Material materials with Módulo de flexión of 7.1 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 8.1 GPa Show Supplier Material materials with Módulo elástico of 8.1 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 170 MPa Show Supplier Material materials with Resistencia a la flexión of 170 MPa | ISO 178 | break, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 106 MPa Show Supplier Material materials with Resistencia a la tracción of 106 MPa | ISO 527 | break, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 11 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 11 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 30 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 30 kJ/m² | ISO 180/1U | unnotched 80*10*4, -30°C |
Taber Abrasion | 23.0 °C | 70 mg/1000cy Show Supplier Material materials with Taber Abrasion of 70 mg/1000cy | SABIC method | CS-17, 1 kg |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | 125°C +/- 2°C | |||
Coeficiente de dilatación térmica | 23.0 °C | 2E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 7E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 7E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Glow Wire Ignition Temperature | 750 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 750 °C | IEC 60695-2-13 | 3.0 mm | |||
Heat deflection temperature, 0.45 MPa | 145 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 145 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 140 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 140 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | UL 746B | |||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | UL 746B | |||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | UL 746B | |||
Temperatura de flexión bajo carga | 140 - 145 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 140 - 145 °C | ||||
Temperatura de reblandecimiento Vicat | 158 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 158 °C | ISO 306 | Rate B/120 | |||
Inflamabilidad | UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 <br> Glow Wire Flammability Index 750°C, passes at: 3mm IEC 60695-2-12 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=103460844- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 23.0 °C | 2.9 [-] Show Supplier Material materials with Constante dieléctrica, 1 MHz of 2.9 [-] | IEC 60250 |
Dielectric constant, 60Hz | 23.0 °C | 2.9 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.9 [-] | IEC 60250 | 50/60 Hz |
Dissipation factor, 1MHz | 23.0 °C | 1E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 1E-3 [-] | IEC 60250 |
Dissipation factor, 50Hz | 23.0 °C | 6E-4 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 6E-4 [-] | IEC 60250 | 50/60 Hz |
Rigidez dieléctrica | 23.0 °C | 18 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 18 kV/mm | IEC 60243-1 | in oil, 3.2 mm, |
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | >, IEC 60093 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | IEC 60093 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.1 % Show Supplier Material materials with Contracción of 0.1 % | SABIC method | 3.2 mm |
Contracción transversal | 23.0 °C | 0.2 % Show Supplier Material materials with Contracción transversal of 0.2 % | SABIC method | 3.2 mm |
Velocidad de flujo del volumen derretido | 16 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 16 cm³/10min | ISO 1133 | MVR at 300°C/10.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Hydroblocks | |
Availability | Europe | |
Processing methods | Mold Temperature: 80 to 120.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |