General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.35 % Show Supplier Material materials with Absorción de agua of 0.35 % | ISO 62-1 | (23°C/saturated) |
Densidad | 23.0 °C | 1.19 g/cm³ Show Supplier Material materials with Densidad of 1.19 g/cm³ | ISO 1183 |
Densidad relativa | 23.0 °C | 1.18 [-] Show Supplier Material materials with Densidad relativa of 1.18 [-] | ASTM D 792 | |
Moisture absorption | 23.0 °C | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | ISO 62 | (23°C / 50% RH) |
Índice límite de óxigeno | 23.0 °C | 35 % Show Supplier Material materials with Índice límite de óxigeno of 35 % |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elongación | 23.0 °C | 6 % Show Supplier Material materials with Elongación of 6 % | ISO 527 | yield, 50 mm/min | ||
Hardness, Ball Indentation | 23.0 °C | 90 MPa Show Supplier Material materials with Hardness, Ball Indentation of 90 MPa | ISO 2039-1 | H358/30 | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 587 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 587 J/m | ASTM D 256 | -50°C | ||
Instrumented Impact, Total Energy | 23.0 °C | 52 J Show Supplier Material materials with Instrumented Impact, Total Energy of 52 J | ASTM D 3763 | 23°C | ||
Módulo de flexión | 23.0 °C | 2.2 GPa Show Supplier Material materials with Módulo de flexión of 2.2 GPa | ISO 178 | 2 mm/min | ||
Módulo elástico | 23.0 °C | 2.1 GPa Show Supplier Material materials with Módulo elástico of 2.1 GPa | ISO 527 | 1 mm/min | ||
Resistencia a la flexión | 23.0 °C | 85 MPa Show Supplier Material materials with Resistencia a la flexión of 85 MPa | ISO 178 | yield, 2 mm/min | ||
Resistencia a la tracción | 23.0 °C | 60 MPa Show Supplier Material materials with Resistencia a la tracción of 60 MPa | ISO 527 | break, 50 mm/min | ||
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 60 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 60 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*3 sp=62mm, -30°C | ||
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 80 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 80 kJ/m² | ISO 180/4A | notched 63.5*12.7*3.2, 23°C, | ||
Resistencia al choque, ensayo Charpy no entallado | ISO 179/1eU | Unnotch Edgew 80*10*3 sp=62mm, 23°C | ||||
Resistencia al choque, ensayo Izod no entallado | ISO 180/1U | unnotched 80*10*3, -30°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | 125°C +/- 2°C | |||
Coeficiente de dilatación térmica | 23.0 °C | 7.2E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7.2E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 7.2E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 7.2E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 825 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 825 °C | IEC 60695-2-13 | 2.3 mm | |||
Heat deflection temperature, 0.45 MPa | 135 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 135 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 124 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 124 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Relative temperature index, electrical | 125 °C Show Supplier Material materials with Relative temperature index, electrical of 125 °C | UL 746B | |||
Relative temperature index, mechanical impact | 115 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 115 °C | UL 746B | |||
Relative temperature index, mechanical strength | 125 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 125 °C | UL 746B | |||
Temperatura de flexión bajo carga | 124 - 135 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 124 - 135 °C | ||||
Temperatura de reblandecimiento Vicat | 142 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 142 °C | ISO 306 | Rate B/120 | |||
Inflamabilidad | UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: ≥3mm UL 94 <br> Glow Wire Ignitability Temperature, 1.0 mm: 825°C IEC 60695-2-13 <br> UV-light, water exposure/immersion: F1- UL 746C <br> UL Recognized, 94-5VB Flame Class Rating: ≥2.5mm UL 94 <br> UL Recognized, 94V-1 Flame Class Rating: ≥0.8mm UL 94 <br> UL Recognized, 94HB Flame Class Rating: ≥0.7mm UL 94 <br> Glow Wire Ignitability Temperature, 1.5 mm: 825°C IEC 60695-2-13 <br> Glow Wire Flammability Index, 1.5 mm: 960°C IEC 60695-2-12 <br> Glow Wire Flammability Index, 1.0 mm: 960°C IEC 60695-2-12 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=103803129- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 23.0 °C | 2.7 [-] Show Supplier Material materials with Constante dieléctrica, 1 MHz of 2.7 [-] | IEC 60250 |
Dielectric constant, 60Hz | 23.0 °C | 2.6 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.6 [-] | IEC 60250 | 50/60 Hz |
Dissipation factor, 1MHz | 23.0 °C | 8.5E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 8.5E-3 [-] | IEC 60250 |
Dissipation factor, 50Hz | 23.0 °C | 1E-3 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 1E-3 [-] | IEC 60250 | 50/60 Hz |
High Amp Arc Ignition | 23.0 °C | 0.6 mm Show Supplier Material materials with High Amp Arc Ignition of 0.6 mm | ≥, UL 746A | PLC 1 |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 1 |
Rigidez dieléctrica | 23.0 °C | 16 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 16 kV/mm | IEC 60243-1 | in oil, 3.2 mm, |
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | >, IEC 60093 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | >, IEC 60093 | |
Índice de seguimiento comparativo | 23.0 °C | 3 V Show Supplier Material materials with Índice de seguimiento comparativo of 3 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.4 % Show Supplier Material materials with Contracción of 0.4 % | SABIC method | 3.2 mm |
Contracción transversal | 23.0 °C | 0.4 % Show Supplier Material materials with Contracción transversal of 0.4 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 10 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 10 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Velocidad de flujo del volumen derretido | 9 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 9 cm³/10min | ISO 1133 | MVR at 300°C/1.2 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Wireless Communications, Water Treatment/Filtration, Wearables, Wiring Devices, Washing Machine, Vending Machine, Traffic Management, Swimming Pool/Spa, Photo/Video Camera, Power Manangement, Photovoltaic Components, Refrigerator, Recreational Vehicle, Rail Cabin Interiors, Pump, Power Boat, Respiratory, Rail, Renal and Blood Handling, Semiconductor, Security/Detection, Surgical Devices, Small Appliance, Smart/ID Card, Medical Device, LED Lighting, Monitoring and Imaging, Microwave Oven, Laundry Dryer, Meter Gas, Interior Rail Components, Inverter, Ignition System, Personal Computing, Non-LED Lighting, Oil/Gas, Electronic Components, Enclosures, Enclosure/Housing/Cover, Energy Management, Electronics, Exercise Equipment, Exterior Rail Components, Freezer, Furnace/Heater, EV Infrastructure, Lab Ware and Clinical Diagnostics, Lawn/Garden, Individual Equiptment, Industrial Material Handling, Head Protection, Fuel Cell, Heavy Vehicles, Air Cabin Interiors, Aircraft Seating, Air Conditioning, Audio, ATM/Ticket Machine, Building Accessory, Circuit Protection, Data Transfer, Data Management, Building Element, Battery System, Cladding, Document Handling, Defense Vehicles, Display, Displays, Wire & cable, Irrigation | |
Availability | Asia | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |