General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.35 % Show Supplier Material materials with Absorción de agua of 0.35 % | ISO 62-1 | (23°C/saturated) |
Densidad | 23.0 °C | 1.2 g/cm³ Show Supplier Material materials with Densidad of 1.2 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | ISO 62 | (23°C / 50% RH) |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elongación | 23.0 °C | 6 % Show Supplier Material materials with Elongación of 6 % | ISO 527 | yield, 50 mm/min | ||
Hardness, Ball Indentation | 23.0 °C | 95 MPa Show Supplier Material materials with Hardness, Ball Indentation of 95 MPa | ISO 2039-1 | H358/30 | ||
Módulo de flexión | 23.0 °C | 2.3 GPa Show Supplier Material materials with Módulo de flexión of 2.3 GPa | ISO 178 | 2 mm/min | ||
Módulo elástico | 23.0 °C | 2.4 GPa Show Supplier Material materials with Módulo elástico of 2.4 GPa | ISO 527 | 1 mm/min | ||
Resistencia a la flexión | 23.0 °C | 90 MPa Show Supplier Material materials with Resistencia a la flexión of 90 MPa | ISO 178 | yield, 2 mm/min | ||
Resistencia a la tracción | 23.0 °C | 63 MPa Show Supplier Material materials with Resistencia a la tracción of 63 MPa | ISO 527 | yield, 50 mm/min | ||
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 60 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 60 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*3 sp=62mm, 23°C | ||
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 60 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 60 kJ/m² | ISO 180/1A | 80*10*3, 23°C | ||
Resistencia al choque, ensayo Charpy no entallado | ISO 179/1eU | Unnotch Edgew 80*10*3 sp=62mm, 23°C | ||||
Resistencia al choque, ensayo Izod no entallado | ISO 180/1U | 80*10*3, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | 125°C +/- 2°C | |
Coeficiente de dilatación térmica | 23.0 °C | 7E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7E-5 1/K | ISO 11359-2 | 23°C to 80°C |
Heat deflection temperature, 0.45 MPa | 133 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 133 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |
Heat deflection temperature, 1.80 MPa | 121 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 121 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |
Temperatura de flexión bajo carga | 121 - 133 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 121 - 133 °C | ||
Temperatura de reblandecimiento Vicat | 139 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 139 °C | ISO 306 | Rate B/50 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Índice de seguimiento comparativo | 23.0 °C | 275 V Show Supplier Material materials with Índice de seguimiento comparativo of 275 V | IEC 60112 | |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | SABIC method | on tensile bar |
Velocidad de flujo del volumen derretido | 26 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 26 cm³/10min | ISO 1133 | MVR at 300°C/1.2 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Data Management, Audio, Circuit Protection, LED Lighting, Personal Computing, Non-LED Lighting, Rear/Signal Lighting | |
Availability | Europe | |
Processing methods | Middle - Zone 2 Temperature: 270 to 290.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |