Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.13 % Show Supplier Material materials with Absorción de agua of 0.13 % | ISO 62-1 | (23°C/saturated) |
Densidad relativa | 23.0 °C | 1.1 [-] Show Supplier Material materials with Densidad relativa of 1.1 [-] | ASTM D 792 | |
Moisture absorption | 23.0 °C | 0.02 % Show Supplier Material materials with Moisture absorption of 0.02 % | ISO 62 | (23°C / 50% RH) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 7.3 % Show Supplier Material materials with Elongación of 7.3 % | ASTM D 638 | brk, Type I, 50 mm/min |
Módulo de flexión | 23.0 °C | 2.8 GPa Show Supplier Material materials with Módulo de flexión of 2.8 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Módulo elástico | 23.0 °C | 3.1 GPa Show Supplier Material materials with Módulo elástico of 3.1 GPa | ASTM D 638 | 50 mm/min |
Resistencia a la flexión | 23.0 °C | 98 MPa Show Supplier Material materials with Resistencia a la flexión of 98 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Resistencia a la tracción | 23.0 °C | 49 MPa Show Supplier Material materials with Resistencia a la tracción of 49 MPa | ASTM D 638 | brk, Type I, 50 mm/min |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 7.4E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7.4E-5 1/K | ISO 11359-2 | -40°C to 40°C |
Coeficiente de dilatación térmica transversal | 23.0 °C | 7.4E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 7.4E-5 1/K | ISO 11359-2 | -40°C to 40°C |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 1.00E+14 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+14 Ω | IEC 60093 |
Volume resistivity | 23.0 °C | 4.00E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 4.00E+16 Ω·cm | IEC 60093 | |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | SABIC method | 3.2 mm |
Velocidad de flujo del volumen derretido | 34 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 34 cm³/10min | ISO 1133 | MVR at 280°C/2.16 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Displays, Washing Machine | |
Availability | Europe | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |