General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.2 % Show Supplier Material materials with Absorción de agua of 0.2 % | ISO 62-1 | (23°C/saturated) |
Densidad | 23.0 °C | 1.2 g/cm³ Show Supplier Material materials with Densidad of 1.2 g/cm³ | ISO 1183 |
Densidad relativa | 23.0 °C | 1.19 [-] Show Supplier Material materials with Densidad relativa of 1.19 [-] | ASTM D 792 | |
Moisture absorption | 23.0 °C | 0.1 % Show Supplier Material materials with Moisture absorption of 0.1 % | ISO 62 | (23°C / 50% RH) |
Índice límite de óxigeno | 23.0 °C | 34 % Show Supplier Material materials with Índice límite de óxigeno of 34 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 90 % Show Supplier Material materials with Elongación of 90 % | ISO 527 | break, 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 175 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 175 J/m | ASTM D 256 | notched, -30°C |
Instrumented Impact, Total Energy | 23.0 °C | 65 J Show Supplier Material materials with Instrumented Impact, Total Energy of 65 J | ASTM D 3763 | 23°C |
Módulo de flexión | 23.0 °C | 2.5 GPa Show Supplier Material materials with Módulo de flexión of 2.5 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 2.6 GPa Show Supplier Material materials with Módulo elástico of 2.6 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 96 MPa Show Supplier Material materials with Resistencia a la flexión of 96 MPa | ISO 178 | yield, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 65 MPa Show Supplier Material materials with Resistencia a la tracción of 65 MPa | ISO 527 | yield, 50 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 22 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 22 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, 23°C |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 25 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 25 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | Pass | IEC 60695-10-2 | 75°C +/- 2°C | |||
Coeficiente de dilatación térmica | 23.0 °C | 7.5E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7.5E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 7.5E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 7.5E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Conductividad térmica | 23.0 °C | 0.2 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.2 W/(m·K) | ISO 8302 | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | IEC 60695-2-12 | 0.75 mm | |||
Glow Wire Ignition Temperature | 800 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 800 °C | IEC 60695-2-13 | 0.75 mm | |||
Heat deflection temperature, 0.45 MPa | 100 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 100 °C | ASTM D 648 | 3.2 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 93 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 93 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 90 °C Show Supplier Material materials with Relative temperature index, electrical of 90 °C | UL 746B | |||
Relative temperature index, mechanical impact | 90 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 90 °C | UL 746B | |||
Relative temperature index, mechanical strength | 90 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 90 °C | UL 746B | |||
Temperatura de flexión bajo carga | 93 - 100 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 93 - 100 °C | ||||
Temperatura de reblandecimiento Vicat | 110 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 110 °C | ISO 306 | Rate B/50 | |||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101674340- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=474277- - <br> UL Recognized, 94-5VA Flame Class Rating: ≥3mm UL 94 <br> UL Recognized, 94-5VB Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.75mm UL 94 <br> UL Recognized, 94V-1 Flame Class Rating: ≥0.6mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> Glow Wire Ignitability Temperature, 1.5 mm: 800°C IEC 60695-2-13 <br> Glow Wire Flammability Index, 1.5 mm: 960°C IEC 60695-2-12 <br> UV-light, water exposure/immersion: F2- UL 746C <br> Glow Wire Flammability Index 960°C, passes at, by VDE: 0.75mm IEC 60695-2-12 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 0.75 mm Show Supplier Material materials with High Amp Arc Ignition of 0.75 mm | ≥, UL 746A | PLC 0 |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 1 |
Rigidez dieléctrica | 23.0 °C | 25 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 25 kV/mm | IEC 60243-1 | in oil, 1.6 mm |
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | >, IEC 60093 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | >, IEC 60093 |
Índice de seguimiento comparativo | 23.0 °C | 3 V Show Supplier Material materials with Índice de seguimiento comparativo of 3 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.4 % Show Supplier Material materials with Contracción of 0.4 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 18 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 18 g/10min | ASTM D 1238 | 260°C/2.16 kgf | |
Velocidad de flujo del volumen derretido | 15 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 15 cm³/10min | ISO 1133 | MVR at 260°C/2.16 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Audio, Auto Aftermarket, Circuit Protection, Battery Cell, Battery Pack, Building Accessory, Air Cabin Interiors, Air Filtration, Air Conditioning, Data Transfer, Data Management, Displays, Dishwasher, Document Handling, Heavy Vehicles, Game Player, Fixture Bath/Shower, Fluid Delivery, EV Infrastructure, EV/HEV Charging System, Electronic Components, Enclosure/Housing/Cover, Energy Management, Electronics, Enclosures, Wiring Devices, Wearables, Wireless Communications, Washing Machine, Vacuum Cleaner, Toy, Small Appliance, Smart/ID Card, Surgical Devices, Respiratory, Rail, Security/Detection, Rail Window Glazing, Refrigerator, Rail Seating, Power Manangement, Photo/Video Camera, Pharmaceutical Packaging & Drug Delivery, Personal Computing, Non-LED Lighting, Personal Care, Monitoring and Imaging, Medical Facility Infrastructure, Interior Rail Components, Meter Gas, LED Lighting, Medical Device, Wire & cable | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80 to 90.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |