Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 120 % Show Supplier Material materials with Elongación of 120 % | ASTM D 638 | brk, Type I, 50 mm/min |
Módulo de flexión | 23.0 °C | 1.3 GPa Show Supplier Material materials with Módulo de flexión of 1.3 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Módulo elástico | 23.0 °C | 1.2 GPa Show Supplier Material materials with Módulo elástico of 1.2 GPa | ASTM D 638 | 50 mm/min |
Resistencia a la flexión | 23.0 °C | 49 MPa Show Supplier Material materials with Resistencia a la flexión of 49 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Resistencia a la tracción | 23.0 °C | 33 MPa Show Supplier Material materials with Resistencia a la tracción of 33 MPa | ASTM D 638 | brk, Type I, 50 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 587 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 587 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 0.45 MPa | 112 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 112 °C | ASTM D 648 | 3.2 mm, unannealed |
Heat deflection temperature, 1.80 MPa | 85 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 85 °C | ASTM D 648 | 3.2mm, unannealed |
Temperatura de flexión bajo carga | 85 - 112 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 85 - 112 °C | |
Temperatura de reblandecimiento Vicat | 85 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 85 °C | ASTM D 1525 | Rate B/50 |
Technological properties
Property | ||
---|---|---|
Application areas | Heavy Vehicles, Long Distance Coach, Recreational Vehicle | |
Availability | Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |