General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.16 % Show Supplier Material materials with Absorción de agua of 0.16 % | ASTM D 570 | (23°C/24hrs) |
Densidad relativa | 23.0 °C | 1.51 [-] Show Supplier Material materials with Densidad relativa of 1.51 [-] | ASTM D 792 |
Índice límite de óxigeno | 23.0 °C | 50 % Show Supplier Material materials with Índice límite de óxigeno of 50 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 3 % Show Supplier Material materials with Elongación of 3 % | ASTM D 638 | brk, Type I, 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 85 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 85 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 427 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 427 J/m | ASTM D 4812 | 23°C |
Módulo de flexión | 23.0 °C | 9 GPa Show Supplier Material materials with Módulo de flexión of 9 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Módulo elástico | 23.0 °C | 9.3 GPa Show Supplier Material materials with Módulo elástico of 9.3 GPa | ASTM D 638 | 5 mm/min |
Resistencia a la flexión | 23.0 °C | 227 MPa Show Supplier Material materials with Resistencia a la flexión of 227 MPa | ASTM D 790 | brk, 2.6 mm/min, 100 mm span |
Resistencia a la tracción | 23.0 °C | 168 MPa Show Supplier Material materials with Resistencia a la tracción of 168 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 85 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 85 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.98E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.98E-5 1/K | ASTM E 831 | -20°C to 150°C | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 900 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 900 °C | IEC 60695-2-13 | 2.0 mm | |||
Heat deflection temperature, 0.45 MPa | 212 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 212 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 210 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 210 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Relative temperature index, electrical | 180 °C Show Supplier Material materials with Relative temperature index, electrical of 180 °C | UL 746B | |||
Relative temperature index, mechanical impact | 170 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 170 °C | UL 746B | |||
Relative temperature index, mechanical strength | 180 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 180 °C | UL 746B | |||
Temperatura de flexión bajo carga | 210 - 212 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 210 - 212 °C | ||||
Temperatura de reblandecimiento Vicat | 227 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 227 °C | ASTM D 1525 | Rate B/50 | |||
Inflamabilidad | UL Recognized, 94V-0 Flame Class Rating: ≥0.25mm UL 94 <br> NBS Smoke Density, Flaming, Ds 4 min: 1.6- ASTM E 662 <br> UL Recognized, 94-5VA Flame Class Rating: ≥1.2mm UL 94 <br> UV-light, water exposure/immersion: F1- UL 746C <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221099- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=470961- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Factor de disipación | 23.0 °C | 5.3E-3 [-] Show Supplier Material materials with Factor de disipación of 5.3E-3 [-] | ASTM D 150 | 2450 MHz |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 3 |
High Volt Arc Track Rate | 23.0 °C | 3 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 3 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 1 |
Rigidez dieléctrica | 23.0 °C | 24.8 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 24.8 kV/mm | ASTM D 149 | in air, 1.6 mm |
Volume resistivity | 23.0 °C | 3.00E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 3.00E+16 Ω·cm | ASTM D 257 |
Índice de seguimiento comparativo | 23.0 °C | 4 V Show Supplier Material materials with Índice de seguimiento comparativo of 4 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.2 % Show Supplier Material materials with Contracción of 0.2 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Aircraft Seating, Air Cabin Interiors, Auto Aftermarket, Medical Facility Infrastructure, Surgical Devices | |
Availability | Europe,Asia,Americas | |
Processing methods | Middle - Zone 2 Temperature: 340 to 400.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |