General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.71 g/cm³ Show Supplier Material materials with Densidad of 1.71 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2.4 % Show Supplier Material materials with Elongación of 2.4 % | ASTM D 638 | break |
Módulo de flexión | 23.0 °C | 19.4 GPa Show Supplier Material materials with Módulo de flexión of 19.4 GPa | ASTM D 790 |
Módulo elástico | 23.0 °C | 22.4 GPa Show Supplier Material materials with Módulo elástico of 22.4 GPa | ASTM D 638 | 50 mm/min |
Resistencia a la flexión | 23.0 °C | 365 MPa Show Supplier Material materials with Resistencia a la flexión of 365 MPa | ASTM D 790 |
Resistencia a la tracción | 23.0 °C | 210 MPa Show Supplier Material materials with Resistencia a la tracción of 210 MPa | ASTM D 638 | break |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 170 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 170 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 210 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 210 °C | ASTM D 648 | 3.2mm, unannealed | |
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | UL 746B | |
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | UL 746B | |
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | UL 746B | |
Temperatura de flexión bajo carga | 210 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 210 °C | ||
Inflamabilidad | UL Recognized, 94HB Flame Class Rating: 1.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=103093414- - |
Technological properties
Property | ||
---|---|---|
Application areas | Washing Machine, Wiring Devices | |
Availability | Europe,Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |