General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.26 g/cm³ Show Supplier Material materials with Densidad of 1.26 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 5 % Show Supplier Material materials with Elongación of 5 % | ASTM D 638 | yield |
Módulo de flexión | 23.0 °C | 2.2 GPa Show Supplier Material materials with Módulo de flexión of 2.2 GPa | ASTM D 790 |
Resistencia a la flexión | 23.0 °C | 84 MPa Show Supplier Material materials with Resistencia a la flexión of 84 MPa | ASTM D 790 |
Resistencia a la tracción | 23.0 °C | 55 MPa Show Supplier Material materials with Resistencia a la tracción of 55 MPa | ASTM D 638 | yield |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 640 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 640 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 1.00E+10 - 1.00E+12 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+10 - 1.00E+12 Ω | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.53 % Show Supplier Material materials with Contracción of 0.53 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Rail Cabin Interiors, Monitoring and Imaging, Personal Computing, Document Handling, Data Management, Lab Ware and Clinical Diagnostics, Electronic Components | |
Availability | Europe,Asia,Americas | |
Processing methods | Middle - Zone 2 Temperature: 210 to 220.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |