General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.3 % Show Supplier Material materials with Absorción de agua of 0.3 % | ISO 62-1 | (23°C/saturated) |
Densidad | 23.0 °C | 1.2 g/cm³ Show Supplier Material materials with Densidad of 1.2 g/cm³ | ISO 1183 |
Densidad relativa | 23.0 °C | 1.2 [-] Show Supplier Material materials with Densidad relativa of 1.2 [-] | ASTM D 792 | |
Moisture absorption | 23.0 °C | 0.23 % Show Supplier Material materials with Moisture absorption of 0.23 % | ISO 62 | (23°C / 50% RH) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 6.5 % Show Supplier Material materials with Elongación of 6.5 % | ISO 527 | yield, 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 115 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 115 J/m | ASTM D 256 | notched, 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 68 J Show Supplier Material materials with Instrumented Impact, Total Energy of 68 J | ASTM D 3763 | 23°C |
Módulo de flexión | 23.0 °C | 2.5 GPa Show Supplier Material materials with Módulo de flexión of 2.5 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 2.6 GPa Show Supplier Material materials with Módulo elástico of 2.6 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 100 MPa Show Supplier Material materials with Resistencia a la flexión of 100 MPa | ISO 178 | yield, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 70 MPa Show Supplier Material materials with Resistencia a la tracción of 70 MPa | ISO 527 | yield, 50 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 10 kJ/m² | ISO 180/1A | notched 80*10*4, -30°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 6E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 6E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 6E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 875 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 875 °C | IEC 60695-2-13 | 3.0 mm | |||
Heat deflection temperature, 0.45 MPa | 155 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 155 °C | ASTM D 648 | 3.2 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 142 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 142 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 150 °C Show Supplier Material materials with Relative temperature index, electrical of 150 °C | UL 746B | |||
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | UL 746B | |||
Relative temperature index, mechanical strength | 150 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 150 °C | UL 746B | |||
Temperatura de flexión bajo carga | 142 - 155 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 142 - 155 °C | ||||
Temperatura de reblandecimiento Vicat | 162 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 162 °C | ISO 306 | Rate B/120 | |||
Inflamabilidad | UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100321023- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 3 |
Índice de seguimiento comparativo | 23.0 °C | 3 V Show Supplier Material materials with Índice de seguimiento comparativo of 3 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.6 % Show Supplier Material materials with Contracción of 0.6 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 46 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 46 g/10min | ASTM D 1238 | 330°C/2.16 kgf | |
Velocidad de flujo del volumen derretido | 43 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 43 cm³/10min | ISO 1133 | MVR at 330°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | LED Lighting, Safety Glasses, Respiratory, Rear/Signal Lighting, Wireless Communications, Travel Suitcase, Data Transfer, Cladding, Fog Lamp, Forward Lighting | |
Availability | Europe,Asia,Americas | |
Processing methods | Front - Zone 3 Temperature: 290 to 330.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |