General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad relativa | 23.0 °C | 1.48 [-] Show Supplier Material materials with Densidad relativa of 1.48 [-] | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 3 % Show Supplier Material materials with Elongación of 3 % | ASTM D 638 | brk, Type I, 5 mm/min |
Módulo de flexión | 23.0 °C | 7.1 GPa Show Supplier Material materials with Módulo de flexión of 7.1 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Resistencia a la flexión | 23.0 °C | 193 MPa Show Supplier Material materials with Resistencia a la flexión of 193 MPa | ASTM D 790 | brk, 2.6 mm/min, 100 mm span |
Resistencia a la tracción | 23.0 °C | 129 MPa Show Supplier Material materials with Resistencia a la tracción of 129 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 212 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 212 °C | ASTM D 648 | 6.4 mm, unannealed | |
Relative temperature index, electrical | 105 °C Show Supplier Material materials with Relative temperature index, electrical of 105 °C | UL 746B | |
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |
Relative temperature index, mechanical strength | 105 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 105 °C | UL 746B | |
Temperatura de flexión bajo carga | 212 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 212 °C | ||
Inflamabilidad | UL Recognized, 94V-0 Flame Class Rating: 1.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=524104- - |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 10.3 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 10.3 g/10min | ASTM D 1238 | 337°C/6.6 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Document Handling | |
Availability | Asia,Americas | |
Processing methods | Screw Speed: 40 to 70.0rpm | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |