General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.11 % Show Supplier Material materials with Absorción de agua of 0.11 % | ASTM D 570 | (23°C/24hrs) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 1.2 % Show Supplier Material materials with Elongación of 1.2 % | ASTM D 638 | brk, Type I, 5 mm/min |
Módulo de flexión | 23.0 °C | 8.8 GPa Show Supplier Material materials with Módulo de flexión of 8.8 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Resistencia a la flexión | 23.0 °C | 113 MPa Show Supplier Material materials with Resistencia a la flexión of 113 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Resistencia a la tracción | 23.0 °C | 82 MPa Show Supplier Material materials with Resistencia a la tracción of 82 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Taber Abrasion | 23.0 °C | 33 mg/1000cy Show Supplier Material materials with Taber Abrasion of 33 mg/1000cy | ASTM D 1044 | CS-17, 1 kg |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.62E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.62E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Heat deflection temperature, 1.80 MPa | 212 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 212 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Relative temperature index, electrical | 105 °C Show Supplier Material materials with Relative temperature index, electrical of 105 °C | UL 746B | |||
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |||
Relative temperature index, mechanical strength | 105 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 105 °C | UL 746B | |||
Temperatura de flexión bajo carga | 212 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 212 °C | ||||
Temperatura de reblandecimiento Vicat | 233 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 233 °C | ASTM D 1525 | Rate B/50 | |||
Inflamabilidad | UL Recognized, 94V-0 Flame Class Rating: 0.84mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221109- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Índice de seguimiento comparativo | 23.0 °C | 4 V Show Supplier Material materials with Índice de seguimiento comparativo of 4 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.2 % Show Supplier Material materials with Contracción of 0.2 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Enclosure/Housing/Cover, Enclosures, Circuit Protection, Wireless Communications, Pharmaceutical Packaging & Drug Delivery | |
Availability | Europe,Asia,Americas | |
Processing methods | Vent Depth: 0.025 to 0.076mm | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |