General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.15 % Show Supplier Material materials with Absorción de agua of 0.15 % | ISO 62-1 | (23°C/saturated) |
Densidad | 23.0 °C | 1.09 g/cm³ Show Supplier Material materials with Densidad of 1.09 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.06 % Show Supplier Material materials with Moisture absorption of 0.06 % | ISO 62 | (23°C / 50% RH) |
Índice límite de óxigeno | 23.0 °C | 34 % Show Supplier Material materials with Índice límite de óxigeno of 34 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 4 % Show Supplier Material materials with Elongación of 4 % | ISO 527 | yield, 50 mm/min |
Módulo de flexión | 23.0 °C | 2.4 GPa Show Supplier Material materials with Módulo de flexión of 2.4 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 2.5 GPa Show Supplier Material materials with Módulo elástico of 2.5 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 98 MPa Show Supplier Material materials with Resistencia a la flexión of 98 MPa | ISO 178 | yield, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 64 MPa Show Supplier Material materials with Resistencia a la tracción of 64 MPa | ISO 527 | yield, 50 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 26 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 26 kJ/m² | ISO 179/1eA | V-notch Edgew, 23°C, 80*10*4 sp=62mm |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 9 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 9 kJ/m² | ISO 180/1A | notched 80*10*4, -30°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | Pass | IEC 60695-10-2 | 125°C +/- 2°C | |||
Coeficiente de dilatación térmica | 23.0 °C | 8.2E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 8.2E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 9.4E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 9.4E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Heat deflection temperature, 0.45 MPa | 129 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 129 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 114 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 114 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | UL 746B | |||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | UL 746B | |||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | UL 746B | |||
Temperatura de flexión bajo carga | 114 - 129 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 114 - 129 °C | ||||
Temperatura de reblandecimiento Vicat | 149 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 149 °C | ISO 306 | Rate B/50 | |||
Inflamabilidad | UL Recognized, 94V-1 Flame Class Rating: 1.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100158340- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 23.0 °C | 2.6 [-] Show Supplier Material materials with Constante dieléctrica, 1 MHz of 2.6 [-] | IEC 60250 |
Dissipation factor, 1MHz | 23.0 °C | 1.7E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 1.7E-3 [-] | IEC 60250 |
Rigidez dieléctrica | 23.0 °C | 46 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 46 kV/mm | IEC 60243-1 | shorttime, 1.0mm |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo del volumen derretido | 9 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 9 cm³/10min | ISO 1133 | MVR at 280°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Pipe/Fitting, Enclosures | |
Availability | Europe | |
Processing methods | Drying Time: 2 to 3.0hrs | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |