General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.23 % Show Supplier Material materials with Absorción de agua of 0.23 % | ISO 62-1 | (23°C/saturated) |
Densidad | 23.0 °C | 1.56 g/cm³ Show Supplier Material materials with Densidad of 1.56 g/cm³ | ISO 1183 |
Densidad relativa | 23.0 °C | 1.56 [-] Show Supplier Material materials with Densidad relativa of 1.56 [-] | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.09 % Show Supplier Material materials with Moisture absorption of 0.09 % | ISO 62 | (23°C / 50% RH) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2 % Show Supplier Material materials with Elongación of 2 % | ISO 527 | yield, 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 72 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 72 J/m | ASTM D 256 | 0°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 570 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 570 J/m | ASTM D 4812 | 23°C |
Módulo de flexión | 23.0 °C | 10 GPa Show Supplier Material materials with Módulo de flexión of 10 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 11 GPa Show Supplier Material materials with Módulo elástico of 11 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 175 MPa Show Supplier Material materials with Resistencia a la flexión of 175 MPa | ISO 178 | yield, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 108 MPa Show Supplier Material materials with Resistencia a la tracción of 108 MPa | ISO 527 | yield, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 8 kJ/m² | ISO 180/1A | notched 80*10*4, -30°C |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 37 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 37 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | 125°C +/- 2°C | |||
Coeficiente de dilatación térmica | 23.0 °C | 2.4E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.4E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 8E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 8E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 750 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 750 °C | IEC 60695-2-13 | 0.8 mm | |||
Heat deflection temperature, 1.80 MPa | 205 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 205 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | UL 746B | |||
Relative temperature index, mechanical impact | 125 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 125 °C | UL 746B | |||
Relative temperature index, mechanical strength | 140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C | UL 746B | |||
Temperatura de flexión bajo carga | 205 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 205 °C | ||||
Temperatura de reblandecimiento Vicat | 200 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 200 °C | ISO 306 | Rate B/50 | |||
Inflamabilidad | UL Recognized, 94V-0 Flame Class Rating: ≥0.8mm UL 94 <br> UL Recognized, 94-5VB Flame Class Rating: ≥3mm UL 94 <br> Glow Wire Ignitability Temperature, 1.5 mm: 775°C IEC 60695-2-13 <br> Glow Wire Ignitability Temperature, 1.0 mm: 750°C IEC 60695-2-13 <br> Glow Wire Flammability Index, 1.5 mm: 960°C IEC 60695-2-12 <br> Glow Wire Flammability Index, 1.0 mm: 960°C IEC 60695-2-12 <br> Glow Wire Flammability Index, 0.8 mm: 960°C IEC 60695-2-12 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100737680- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 0.8 mm Show Supplier Material materials with High Amp Arc Ignition of 0.8 mm | ≥, UL 746A | PLC 0 |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 0 |
Volume resistivity | 23.0 °C | 1.00E+14 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+14 Ω·cm | ASTM D 257 |
Índice de seguimiento comparativo | 23.0 °C | 0 V Show Supplier Material materials with Índice de seguimiento comparativo of 0 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.28 % Show Supplier Material materials with Contracción of 0.28 % | SABIC method | 3.2 mm |
Contracción transversal | 23.0 °C | 0.57 % Show Supplier Material materials with Contracción transversal of 0.57 % | SABIC method | 3.2 mm |
Velocidad de flujo del volumen derretido | 16 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 16 cm³/10min | ISO 1133 | MVR at 250°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, EV Infrastructure, Data Transfer, Data Management, Inverter, Personal Computing, Power Manangement, Wireless Communications | |
Availability | Europe,Asia,Americas | |
Processing methods | Melt Temperature: 245 to 260.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |