General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.15 % Show Supplier Material materials with Absorción de agua of 0.15 % | ISO 62-1 | (23°C/saturated) |
Densidad | 23.0 °C | 1.45 g/cm³ Show Supplier Material materials with Densidad of 1.45 g/cm³ | ISO 1183 |
Densidad relativa | 23.0 °C | 1.45 [-] Show Supplier Material materials with Densidad relativa of 1.45 [-] | ASTM D 792 | |
Moisture absorption | 23.0 °C | 0.07 % Show Supplier Material materials with Moisture absorption of 0.07 % | ISO 62 | (23°C / 50% RH) |
Índice límite de óxigeno | 23.0 °C | 31 % Show Supplier Material materials with Índice límite de óxigeno of 31 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 3 % Show Supplier Material materials with Elongación of 3 % | ISO 527 | break, 5 mm/min |
Flexural strain | 23.0 °C | 3 % Show Supplier Material materials with Flexural strain of 3 % | ISO 178 | break, 2 mm/min |
Hardness, Ball Indentation | 23.0 °C | 128 MPa Show Supplier Material materials with Hardness, Ball Indentation of 128 MPa | ISO 2039-1 | H358/30 |
Hardness, Rockwell R | 23.0 °C | 98 [-] Show Supplier Material materials with Hardness, Rockwell R of 98 [-] | ISO 2039-2 |
Impact strength, Izod notched, ASTM | 23.0 °C | 50 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 50 J/m | ASTM D 256 | 0°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 360 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 360 J/m | ASTM D 4812 | unnotched, -30°C |
Módulo de flexión | 23.0 °C | 6.4 GPa Show Supplier Material materials with Módulo de flexión of 6.4 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 7.5 GPa Show Supplier Material materials with Módulo elástico of 7.5 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 130 MPa Show Supplier Material materials with Resistencia a la flexión of 130 MPa | ISO 178 | break, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 80 MPa Show Supplier Material materials with Resistencia a la tracción of 80 MPa | ISO 527 | break, 5 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | ISO 179/2C | -30°C |
Resistencia al choque, ensayo Charpy no entallado | 23.0 °C | 25 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 25 kJ/m² | ISO 179/2C | -30°C |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 6 kJ/m² | ISO 180/1A | notched 80*10*4, -30°C |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 30 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 30 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | 125°C +/- 2°C | |
Coeficiente de dilatación térmica | 23.0 °C | 4.2E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 4.2E-5 1/K | ISO 11359-2 | 23°C to 150°C |
Coeficiente de dilatación térmica transversal | 23.0 °C | 1.73E-4 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 1.73E-4 1/K | ISO 11359-2 | 23°C to 150°C |
Heat deflection temperature, 0.45 MPa | 220 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 220 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |
Heat deflection temperature, 1.80 MPa | 200 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 200 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Temperatura de flexión bajo carga | 200 - 220 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 200 - 220 °C | ||
Temperatura de reblandecimiento Vicat | 205 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 205 °C | ISO 306 | Rate B/120 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 23.0 °C | 3.7 [-] Show Supplier Material materials with Constante dieléctrica, 1 MHz of 3.7 [-] | IEC 60250 |
Dissipation factor, 1MHz | 23.0 °C | 0.15 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 0.15 [-] | IEC 60250 |
Rigidez dieléctrica | 23.0 °C | 28 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 28 kV/mm | IEC 60243-1 | in oil, 0.8 mm |
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | >, IEC 60093 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | IEC 60093 | |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.3 % Show Supplier Material materials with Contracción of 0.3 % | SABIC method | on tensile bar |
Melt viscosity | 23.0 °C | 150 Pa·s Show Supplier Material materials with Melt viscosity of 150 Pa·s | ISO 11443 | 260°C, 1500 sec-1 |
Velocidad de flujo de la masa derretida | 24 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 24 g/10min | ASTM D 1238 | 265°C/5.0 kgf | |
Velocidad de flujo del volumen derretido | 18 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 18 cm³/10min | ISO 1133 | MVR at 265°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Coil bobbin, Electronic Components, Enclosures, Heavy Vehicles, Lab Ware and Clinical Diagnostics, EV Infrastructure, Displays, Wireless Communications, Personal Computing, Respiratory | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 110 to 120.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |