Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.13 % Show Supplier Material materials with Absorción de agua of 0.13 % | ISO 62-1 | (23°C/saturated) |
Densidad | 23.0 °C | 1.25 g/cm³ Show Supplier Material materials with Densidad of 1.25 g/cm³ | ISO 1183 |
Densidad relativa | 23.0 °C | 1.25 [-] Show Supplier Material materials with Densidad relativa of 1.25 [-] | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.04 % Show Supplier Material materials with Moisture absorption of 0.04 % | ISO 62 | (23°C / 50% RH) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 11 % Show Supplier Material materials with Elongación of 11 % | ASTM D 638 | brk, Type I, 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 205 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 205 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1880 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1880 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 36 J Show Supplier Material materials with Instrumented Impact, Total Energy of 36 J | ASTM D 3763 | 23°C |
Módulo de flexión | 23.0 °C | 3.6 GPa Show Supplier Material materials with Módulo de flexión of 3.6 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Módulo elástico | 23.0 °C | 3.9 GPa Show Supplier Material materials with Módulo elástico of 3.9 GPa | ASTM D 638 | 5 mm/min |
Resistencia a la flexión | 23.0 °C | 87 MPa Show Supplier Material materials with Resistencia a la flexión of 87 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Resistencia a la tracción | 23.0 °C | 37 MPa Show Supplier Material materials with Resistencia a la tracción of 37 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 205 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 205 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 127 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 127 °C | ASTM D 648 | 3.2 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 120 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 120 °C | ASTM D 648 | 3.2mm, unannealed | |
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |
Temperatura de flexión bajo carga | 120 - 127 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 120 - 127 °C | ||
Temperatura de reblandecimiento Vicat | 132 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 132 °C | ISO 306 | Rate B/120 | |
Inflamabilidad | UL Recognized, 94HB Flame Class Rating: ≥0.4mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101619221- - |
Óptico
Property | Value | Comment |
---|---|---|
Transmission | -2.5 % Show Supplier Material materials with Transmission of -2.5 % | <, SABIC method | at 0.4 mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.2 % Show Supplier Material materials with Contracción of 0.2 % | SABIC method | 3.2 mm |
Contracción transversal | 23.0 °C | 0.4 % Show Supplier Material materials with Contracción transversal of 0.4 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 15 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 15 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Velocidad de flujo del volumen derretido | 14 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 14 cm³/10min | ISO 1133 | MVR at 300°C/1.2 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Enclosures, Personal Computing, Photo/Video Camera, Wireless Communications | |
Availability | Asia | |
Processing methods | Vent Depth: 0.025 to 0.076mm | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |