General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.62 g/cm³ Show Supplier Material materials with Densidad of 1.62 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2.8 % Show Supplier Material materials with Elongación of 2.8 % | ASTM D 638 | break |
Módulo de flexión | 23.0 °C | 10.3 GPa Show Supplier Material materials with Módulo de flexión of 10.3 GPa | ASTM D 790 |
Resistencia a la flexión | 23.0 °C | 213 MPa Show Supplier Material materials with Resistencia a la flexión of 213 MPa | ASTM D 790 |
Resistencia a la tracción | 23.0 °C | 147 MPa Show Supplier Material materials with Resistencia a la tracción of 147 MPa | ASTM D 638 | break |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 85 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 85 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 161 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 161 °C | ASTM D 648 | 3.2mm, unannealed | |
Temperatura de flexión bajo carga | 161 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 161 °C | ||
Inflamabilidad | UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101284440- - |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Document Handling | |
Availability | Europe,Americas | |
Processing methods | Back Pressure: 0.2 to 0.3MPa | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |