General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.37 g/cm³ Show Supplier Material materials with Densidad of 1.37 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 3 % Show Supplier Material materials with Elongación of 3 % | ISO 527 | break |
Módulo de flexión | 23.0 °C | 8 GPa Show Supplier Material materials with Módulo de flexión of 8 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 8.6 GPa Show Supplier Material materials with Módulo elástico of 8.6 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 225 MPa Show Supplier Material materials with Resistencia a la flexión of 225 MPa | ISO 178 |
Resistencia a la tracción | 23.0 °C | 165 MPa Show Supplier Material materials with Resistencia a la tracción of 165 MPa | ISO 527 | break |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 8 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 203 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 203 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Temperatura de flexión bajo carga | 203 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 203 °C | ||
Inflamabilidad | UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 <br> UV-light, water exposure/immersion: F2- UL 746C <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=103093422- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Índice de seguimiento comparativo | 23.0 °C | 0 V Show Supplier Material materials with Índice de seguimiento comparativo of 0 V | UL 746A | (UL) {PLC} |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Document Handling, Displays, Data Management, Electronic Components, Enclosure/Housing/Cover, Rail Cabin Interiors, Photo/Video Camera, Oil/Gas, Personal Care, Medical Device, Medical Facility Infrastructure, Wire & cable | |
Availability | Europe,Asia,Americas | |
Processing methods | Middle - Zone 2 Temperature: 250 to 260.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |