Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 50 % Show Supplier Material materials with Elongación of 50 % | ISO 527 | break, 50 mm/min |
Módulo de flexión | 23.0 °C | 2.9 GPa Show Supplier Material materials with Módulo de flexión of 2.9 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 2.9 GPa Show Supplier Material materials with Módulo elástico of 2.9 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 110 MPa Show Supplier Material materials with Resistencia a la flexión of 110 MPa | ISO 178 | yield, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 100 MPa Show Supplier Material materials with Resistencia a la tracción of 100 MPa | ISO 527 | yield, 50 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 5 kJ/m² | ISO 180/1A | notched 80*10*4, -30°C |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 200 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 200 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |
Relative temperature index, electrical | 160 °C Show Supplier Material materials with Relative temperature index, electrical of 160 °C | UL 746B | |
Relative temperature index, mechanical impact | 155 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 155 °C | UL 746B | |
Relative temperature index, mechanical strength | 160 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 160 °C | UL 746B | |
Temperatura de flexión bajo carga | 200 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 200 °C | ||
Inflamabilidad | Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 <br> UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221115- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 60Hz | 23.0 °C | 3.2 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 3.2 [-] | IEC 60250 | 50/60 Hz |
Dissipation factor, 50Hz | 23.0 °C | 2.1E-3 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 2.1E-3 [-] | IEC 60250 | 50/60 Hz |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 3 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 3 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 1 |
Rigidez dieléctrica | 23.0 °C | 18.1 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 18.1 kV/mm | IEC 60243-1 | in oil, 3.2 mm, |
Índice de seguimiento comparativo | 23.0 °C | 4 V Show Supplier Material materials with Índice de seguimiento comparativo of 4 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.4 % Show Supplier Material materials with Contracción of 0.4 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Fused Deposition Modeling (FDM), Enclosure/Housing/Cover, Electronic Components, Air Cabin Interiors, Aerospace, Aircraft Seating, Battery Cell, Data Transfer, Document Handling, Wireless Communications | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 150°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |