General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.16 % Show Supplier Material materials with Absorción de agua of 0.16 % | ASTM D 570 | (23°C/24hrs) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 60 % Show Supplier Material materials with Elongación of 60 % | ASTM D 638 | brk, Type I, 5 mm/min |
Módulo de flexión | 23.0 °C | 3.1 GPa Show Supplier Material materials with Módulo de flexión of 3.1 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Módulo elástico | 23.0 °C | 2.9 GPa Show Supplier Material materials with Módulo elástico of 2.9 GPa | ASTM D 638 | 5 mm/min |
Resistencia a la flexión | 23.0 °C | 137 MPa Show Supplier Material materials with Resistencia a la flexión of 137 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Resistencia a la tracción | 23.0 °C | 99 MPa Show Supplier Material materials with Resistencia a la tracción of 99 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 64 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 64 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 207 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 207 °C | ASTM D 648 | 6.4 mm, unannealed | |
Relative temperature index, electrical | 160 °C Show Supplier Material materials with Relative temperature index, electrical of 160 °C | UL 746B | |
Relative temperature index, mechanical impact | 160 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 160 °C | UL 746B | |
Relative temperature index, mechanical strength | 160 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 160 °C | UL 746B | |
Temperatura de flexión bajo carga | 207 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 207 °C | ||
Inflamabilidad | UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221114- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 3 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 3 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
Rigidez dieléctrica | 23.0 °C | 17.9 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 17.9 kV/mm | ASTM D 149 | in oil, 3.2 mm |
Sheet resistivity, ROA | 23.0 °C | 5.80E+16 Ω Show Supplier Material materials with Sheet resistivity, ROA of 5.80E+16 Ω | ASTM D 257 |
Volume resistivity | 23.0 °C | 1.10E+17 Ω·cm Show Supplier Material materials with Volume resistivity of 1.10E+17 Ω·cm | ASTM D 257 |
Índice de seguimiento comparativo | 23.0 °C | 4 V Show Supplier Material materials with Índice de seguimiento comparativo of 4 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.4 % Show Supplier Material materials with Contracción of 0.4 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Medical Device, LED Lighting, Meter Water, Photovoltaic Components, Semiconductor, Wireless Communications, Audio, Aerospace, Air Cabin Interiors, Electronic Components, Enclosure/Housing/Cover, Energy Management, Enclosures, Industrial Material Handling, Heavy Vehicles | |
Availability | Europe,Asia,Americas | |
Processing methods | Shot to Cylinder Size: 40 to 60.0% | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |