General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad relativa | 23.0 °C | 1.26 [-] Show Supplier Material materials with Densidad relativa of 1.26 [-] | ASTM D 792 | |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 6.5 % Show Supplier Material materials with Elongación of 6.5 % | ISO 527 | yield, 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 55 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 55 J/m | ASTM D 256 |
Módulo de flexión | 23.0 °C | 3.1 GPa Show Supplier Material materials with Módulo de flexión of 3.1 GPa | ISO 178 | 2 mm/min |
Resistencia a la flexión | 23.0 °C | 125 MPa Show Supplier Material materials with Resistencia a la flexión of 125 MPa | ISO 178 | yield, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 95 MPa Show Supplier Material materials with Resistencia a la tracción of 95 MPa | ISO 527 | yield, 50 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 5 kJ/m² | ISO 180/1A | 80*10*4, -30°C |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 180 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 180 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |
Relative temperature index, electrical | 115 °C Show Supplier Material materials with Relative temperature index, electrical of 115 °C | UL 746B | |
Relative temperature index, mechanical impact | 115 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 115 °C | UL 746B | |
Relative temperature index, mechanical strength | 115 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 115 °C | UL 746B | |
Temperatura de flexión bajo carga | 180 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 180 °C | ||
Inflamabilidad | UL Recognized, 94V-2 Flame Class Rating: ≥0.75mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.75mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100397331- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 0.75 mm Show Supplier Material materials with High Amp Arc Ignition of 0.75 mm | ≥, UL 746A | PLC 4 |
Hot-Wire Ignition | 23.0 °C | 0.75 mm Show Supplier Material materials with Hot-Wire Ignition of 0.75 mm | ≥, UL 746A | PLC 0 |
Índice de seguimiento comparativo | 23.0 °C | 4 V Show Supplier Material materials with Índice de seguimiento comparativo of 4 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 26.5 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 26.5 g/10min | ASTM D 1238 | 337°C/6.6 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Circuit Protection, Data Transfer, City, Electronic Components, Enclosures, Forward Lighting, Motorcycle, Non-LED Lighting, Personal Computing | |
Availability | Europe,Asia,Americas | |
Processing methods | Rear - Zone 1 Temperature: 320 to 340.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |