General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2.5 % Show Supplier Material materials with Elongación of 2.5 % | ASTM D 638 | brk, Type I, 5 mm/min |
Módulo de flexión | 23.0 °C | 11.7 GPa Show Supplier Material materials with Módulo de flexión of 11.7 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Módulo elástico | 23.0 °C | 11.7 GPa Show Supplier Material materials with Módulo elástico of 11.7 GPa | ASTM D 638 | 5 mm/min |
Resistencia a la flexión | 23.0 °C | 241 MPa Show Supplier Material materials with Resistencia a la flexión of 241 MPa | ASTM D 790 | brk, 2.6 mm/min, 100 mm span |
Resistencia a la tracción | 23.0 °C | 179 MPa Show Supplier Material materials with Resistencia a la tracción of 179 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.44E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.44E-5 1/K | ASTM E 831 | -20°C to 150°C | ||
Heat deflection temperature, 0.45 MPa | 215 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 215 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 212 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 212 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Relative temperature index, electrical | 170 °C Show Supplier Material materials with Relative temperature index, electrical of 170 °C | UL 746B | |||
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |||
Relative temperature index, mechanical strength | 170 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 170 °C | UL 746B | |||
Temperatura de flexión bajo carga | 212 - 215 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 212 - 215 °C | ||||
Temperatura de reblandecimiento Vicat | 234 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 234 °C | ASTM D 1525 | Rate B/50 | |||
Inflamabilidad | NBS Smoke Density, Flaming, Ds 4 min: 1- ASTM E 662 <br> UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=236985- - <br> Glow Wire Ignitability Temperature, 1.5 mm: 875°C IEC 60695-2-13 <br> Glow Wire Ignitability Temperature, 1.0 mm: 850°C IEC 60695-2-13 <br> Glow Wire Flammability Index, 1.5 mm: 960°C IEC 60695-2-12 <br> Glow Wire Flammability Index, 1.0 mm: 960°C IEC 60695-2-12 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 4 |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
Rigidez dieléctrica | 23.0 °C | 24 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 24 kV/mm | ASTM D 149 | in oil, 1.6 mm |
Volume resistivity | 23.0 °C | 1.50E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 1.50E+16 Ω·cm | ASTM D 257 |
Índice de seguimiento comparativo | 23.0 °C | 5 V Show Supplier Material materials with Índice de seguimiento comparativo of 5 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.1 % Show Supplier Material materials with Contracción of 0.1 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Wiring Devices, Wireless Communications, Swimming Pool/Spa, Structure, Oil/Gas, Medical Device, Monitoring and Imaging, Meter Gas, Photo/Video Camera, EV Infrastructure, Enclosures, Electronic Components, Air Cabin Interiors, Aircraft Seating, Circuit Protection, Data Management, Data Transfer, Document Handling, Defense Vehicles | |
Availability | Europe,Asia,Americas | |
Processing methods | Screw Speed: 40 to 70.0rpm | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |