Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 195 % Show Supplier Material materials with Elongación of 195 % | ASTM D 638 | brk, Type I, 50 mm/min |
Módulo de flexión | 23.0 °C | 1.6 GPa Show Supplier Material materials with Módulo de flexión of 1.6 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Módulo elástico | 23.0 °C | 1.3 GPa Show Supplier Material materials with Módulo elástico of 1.3 GPa | ASTM D 638 | 50 mm/min |
Resistencia a la flexión | 23.0 °C | 51 MPa Show Supplier Material materials with Resistencia a la flexión of 51 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Resistencia a la tracción | 23.0 °C | 32 MPa Show Supplier Material materials with Resistencia a la tracción of 32 MPa | ASTM D 638 | brk, Type I, 50 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 437 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 437 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 8.1E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 8.1E-5 1/K | ASTM E 831 | -40°C to 40°C |
Coeficiente de dilatación térmica transversal | 23.0 °C | 1.12E-4 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 1.12E-4 1/K | ASTM E 831 | -40°C to 40°C |
Heat deflection temperature, 0.45 MPa | 113 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 113 °C | ASTM D 648 | 3.2 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 77 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 77 °C | ASTM D 648 | 3.2mm, unannealed | |
Temperatura de flexión bajo carga | 77 - 113 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 77 - 113 °C | ||
Temperatura de reblandecimiento Vicat | 138 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 138 °C | ASTM D 1525 | Rate B/50 |
Technological properties
Property | ||
---|---|---|
Application areas | Medical Device, Wiring Devices, Hot Water System, EV/HEV Battery, Document Handling | |
Availability | Europe,Asia,Americas | |
Processing methods | Nozzle Temperature: 260 to 290.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |