General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.12 % Show Supplier Material materials with Absorción de agua of 0.12 % | ISO 62-1 | (23°C/saturated) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 3 % Show Supplier Material materials with Elongación of 3 % | ISO 527 | break |
Módulo de flexión | 23.0 °C | 4.2 GPa Show Supplier Material materials with Módulo de flexión of 4.2 GPa | ISO 178 |
Módulo elástico | 23.0 °C | 3.9 GPa Show Supplier Material materials with Módulo elástico of 3.9 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 115 MPa Show Supplier Material materials with Resistencia a la flexión of 115 MPa | ISO 178 | yield, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 60 MPa Show Supplier Material materials with Resistencia a la tracción of 60 MPa | ISO 527 | break, 50 mm/min |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 30 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 30 kJ/m² | ISO 180/1U | unnotched 80*10*4, -30°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 3.8E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3.8E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 7E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 7E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Heat deflection temperature, 0.45 MPa | 132 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 132 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 124 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 124 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Temperatura de flexión bajo carga | 124 - 132 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 124 - 132 °C | ||||
Temperatura de reblandecimiento Vicat | 138 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 138 °C | ISO 306 | Rate B/50 | |||
Inflamabilidad | UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 <br> UV-light, water exposure/immersion: F1- UL 746C <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=228544- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=237019- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 0 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.2 % Show Supplier Material materials with Contracción of 0.2 % | SABIC method | 3.2 mm |
Velocidad de flujo del volumen derretido | 8 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 8 cm³/10min | ISO 1133 | MVR at 280°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Document Handling, Coffee Maker/Espresso Machine, Data Transfer, Air Conditioning, Air Filtration, Building Accessory, Circuit Protection, Enclosure/Housing/Cover, Energy Management, Enclosures, Electronic Components, Fixture Bath/Shower, Furnace/Heater, Hot Water System, Heavy Vehicles, Individual Equiptment, Lab Ware and Clinical Diagnostics, Swimming Pool/Spa, Water Treatment/Filtration, Wiring Devices, Wireless Communications, Medical Device, Meter Gas, Personal Computing, Recreational Vehicle, Pump, Pipe/Fitting, Plumbing, Security/Detection, Respiratory, Sanitary, Small Appliance, Irrigation | |
Availability | Europe,Asia,Americas | |
Processing methods | Screw Speed: 20 to 100.0rpm | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |