General
Property | Temperature | Value |
---|---|---|
Índice límite de óxigeno | 23.0 °C | 46 % Show Supplier Material materials with Índice límite de óxigeno of 46 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 100 % Show Supplier Material materials with Elongación of 100 % | ASTM D 638 | brk, Type I, 50 mm/min |
Módulo de flexión | 23.0 °C | 0.4 GPa Show Supplier Material materials with Módulo de flexión of 0.4 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Resistencia a la tracción | 23.0 °C | 28 MPa Show Supplier Material materials with Resistencia a la tracción of 28 MPa | ASTM D 638 | yld, Type I, 50 mm/min |
Taber Abrasion | 23.0 °C | 26 mg/1000cy Show Supplier Material materials with Taber Abrasion of 26 mg/1000cy | ASTM D 1044 | CS-17, 1 kg |
Aplicaciones térmicas
Property | Value |
---|---|
Inflamabilidad | OSU peak heat release rate (5 minute test): 140kW/m² FAR 25.853 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Rigidez dieléctrica | 23.0 °C | 16.1 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 16.1 kV/mm | ASTM D 149 | in air, 3.2 mm |
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | >, ASTM D 257 |
Volume resistivity | 23.0 °C | 4.10E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 4.10E+16 Ω·cm | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Application areas | Defense Vehicles, Document Handling, Air Cabin Interiors, Enclosures, Exterior Rail Components, Interior Rail Components, Wiring Devices, Wire & cable | |
Availability | Europe,Americas | |
Processing methods | Back Pressure: 0.3 to 0.7MPa | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |