General
Property | Temperature | Value |
---|---|---|
Índice límite de óxigeno | 23.0 °C | 48 % Show Supplier Material materials with Índice límite de óxigeno of 48 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 15 % Show Supplier Material materials with Elongación of 15 % | ISO 527 | yield, 50 mm/min |
Módulo de flexión | 23.0 °C | 0.5 GPa Show Supplier Material materials with Módulo de flexión of 0.5 GPa | ISO 178 | 2 mm/min |
Resistencia a la tracción | 23.0 °C | 20 MPa Show Supplier Material materials with Resistencia a la tracción of 20 MPa | ISO 527 | yield, 50 mm/min |
Taber Abrasion | 23.0 °C | 60 mg/1000cy Show Supplier Material materials with Taber Abrasion of 60 mg/1000cy | SABIC method | CS-17, 1 kg |
Aplicaciones térmicas
Property | Value |
---|---|
Inflamabilidad | UL Compliant, 94V-1 Flame Class Rating: 1.6mm UL 94 by SABIC-IP <br> Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Rigidez dieléctrica | 23.0 °C | 19 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 19 kV/mm | IEC 60243-1 | in oil, 3.2 mm, |
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | IEC 60093 |
Volume resistivity | 23.0 °C | 4.70E+14 Ω·cm Show Supplier Material materials with Volume resistivity of 4.70E+14 Ω·cm | IEC 60093 | |
Technological properties
Property | ||
---|---|---|
Application areas | Defense Vehicles, Document Handling, Air Cabin Interiors, Enclosures, Exterior Rail Components, Interior Rail Components, Wiring Devices, Wire & cable | |
Availability | Europe,Americas | |
Processing methods | Drying Temperature: 105 to 110.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |