General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 70 % Show Supplier Material materials with Elongación of 70 % | ISO 527 | break, 50 mm/min |
Módulo de flexión | 23.0 °C | 2.3 GPa Show Supplier Material materials with Módulo de flexión of 2.3 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 2.1 GPa Show Supplier Material materials with Módulo elástico of 2.1 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 95 MPa Show Supplier Material materials with Resistencia a la flexión of 95 MPa | ISO 178 | yield, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 57 MPa Show Supplier Material materials with Resistencia a la tracción of 57 MPa | ISO 527 | yield, 50 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 17 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 17 kJ/m² | ISO 179/1eA | V-notch Edgew, 23°C, 80*10*4 sp=62mm |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 5 kJ/m² | ISO 180/1A | 80*10*4, -30°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 7.3E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7.3E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 8.3E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 8.3E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Heat deflection temperature, 1.80 MPa | 115 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 115 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Relative temperature index, electrical | 105 °C Show Supplier Material materials with Relative temperature index, electrical of 105 °C | UL 746B | |||
Relative temperature index, mechanical impact | 90 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 90 °C | UL 746B | |||
Relative temperature index, mechanical strength | 105 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 105 °C | UL 746B | |||
Temperatura de flexión bajo carga | 115 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 115 °C | ||||
Temperatura de reblandecimiento Vicat | 140 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 140 °C | ISO 306 | Rate B/120 | |||
Inflamabilidad | UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221150- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 6 mm Show Supplier Material materials with High Amp Arc Ignition of 6 mm | ≥, UL 746A | PLC 4 |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 1 |
Índice de seguimiento comparativo | 23.0 °C | 3 V Show Supplier Material materials with Índice de seguimiento comparativo of 3 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | SABIC method | 3.2 mm |
Velocidad de flujo del volumen derretido | 12 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 12 cm³/10min | ISO 1133 | MVR at 280°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Meter Gas, Ignition System, Monitoring and Imaging, Meter Water, Laundry Dryer, LED Lighting, Medical Device, Personal Computing, Non-LED Lighting, Sanitary, Small Appliance, Security/Detection, Renal and Blood Handling, Refrigerator, Recreational Vehicle, Power Boat, Pipe/Fitting, Pump, Plumbing, Pharmaceutical Packaging & Drug Delivery, Wireless Communications, Wiring Devices, Watch/Jewelry, Water Treatment/Filtration, Wheel Cover, Wearables, Swimming Pool/Spa, Surgical Tray, Vending Machine, Washing Machine, Auto Electrical, Building Accessory, Circuit Protection, Audio, Auto Aftermarket, ATM/Ticket Machine, Amusement Machine, Animal Testing, Aerospace, Coffee Maker/Espresso Machine, Bottles, Building Element, Building/Construction Sheet, Data Management, Doors Hardware/Trim, Conveyor, Dishwasher, Displays, Document Handling, EV Infrastructure, Food Transportation, Furnace/Heater, Fixture Bath/Shower, Lawn/Garden, Lab Ware and Clinical Diagnostics, Heavy Vehicles, Gas/Electric Oven, Hot Water System, Head Protection, Electronic Components, Enclosure/Housing/Cover, Electronics, Enclosures | |
Availability | Americas | |
Processing methods | Middle - Zone 2 Temperature: 260 to 305.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |