General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad relativa | 23.0 °C | 1.38 [-] Show Supplier Material materials with Densidad relativa of 1.38 [-] | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 5 % Show Supplier Material materials with Elongación of 5 % | SABIC - Japan Method | yld, Type I, 10 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 68 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 68 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 331 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 331 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 7 J Show Supplier Material materials with Instrumented Impact, Total Energy of 7 J | ASTM D 3763 | 23°C |
Módulo de flexión | 23.0 °C | 9.1 GPa Show Supplier Material materials with Módulo de flexión of 9.1 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 10.6 GPa Show Supplier Material materials with Módulo elástico of 10.6 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 160 MPa Show Supplier Material materials with Resistencia a la flexión of 160 MPa | ISO 178 | yield, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 115 MPa Show Supplier Material materials with Resistencia a la tracción of 115 MPa | SABIC - Japan Method | brk, Type I, 10 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 4 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4 kJ/m² | ISO 179/2C | 23°C |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 5 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 14 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 14 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 2.1E-5 - 3.3E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.1E-5 - 3.3E-5 1/K | TMA | -30°C to 30°C | ||
Heat deflection temperature, 1.80 MPa | 129 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 129 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | UL 746B | |||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | UL 746B | |||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | UL 746B | |||
Temperatura de flexión bajo carga | 129 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 129 °C | ||||
Temperatura de reblandecimiento Vicat | 140 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 140 °C | ASTM D 1525 | Rate B/50 | |||
Inflamabilidad | UL Recognized, 94-5VB Flame Class Rating: ≥2.3mm UL 94 <br> UL Recognized, 94V-1 Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥3mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=228572- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=237063- - |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.25 % Show Supplier Material materials with Contracción of 0.25 % | SABIC method |
Velocidad de flujo de la masa derretida | 11 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 11 g/10min | ASTM D 1238 | 300°C/2.16 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Document Handling, Data Management, Circuit Protection, Enclosures, Enclosure/Housing/Cover, Electronic Components, Security/Detection, Wireless Communications | |
Availability | Asia | |
Processing methods | Drying Time (Cumulative): 8hrs | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |