General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 30 % Show Supplier Material materials with Elongación of 30 % | ASTM D 638 | brk, Type I, 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 288 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 288 J/m | ASTM D 256 | notched, 23°C |
Módulo de flexión | 23.0 °C | 2.3 GPa Show Supplier Material materials with Módulo de flexión of 2.3 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Resistencia a la flexión | 23.0 °C | 99 MPa Show Supplier Material materials with Resistencia a la flexión of 99 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Resistencia a la tracción | 23.0 °C | 62 MPa Show Supplier Material materials with Resistencia a la tracción of 62 MPa | ASTM D 638 | yld, Type I, 50 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 288 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 288 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 7.2E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7.2E-5 1/K | ASTM E 831 | 0°C to 100°C |
Heat deflection temperature, 0.45 MPa | 154 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 154 °C | ASTM D 648 | 6.4 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 146 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 146 °C | ASTM D 648 | 6.4 mm, unannealed | |
Temperatura de flexión bajo carga | 146 - 154 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 146 - 154 °C |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Gas/Electric Oven, Head Protection, Enclosures, Electronic Components, Data Transfer | |
Availability | Asia,Americas | |
Processing methods | Rear - Zone 1 Temperature: 260 to 305.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |