General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 50 % Show Supplier Material materials with Elongación of 50 % | ASTM D 638 | brk, Type I, 50 mm/min |
Gardner Impact | 23.0 °C | 24 J Show Supplier Material materials with Gardner Impact of 24 J | ASTM D 3029 | -30°C |
Hardness, Rockwell R | 23.0 °C | 113 [-] Show Supplier Material materials with Hardness, Rockwell R of 113 [-] | ASTM D 785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 160 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 160 J/m | ASTM D 256 | -40°C |
Módulo de flexión | 23.0 °C | 2.3 GPa Show Supplier Material materials with Módulo de flexión of 2.3 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Resistencia a la flexión | 23.0 °C | 67 MPa Show Supplier Material materials with Resistencia a la flexión of 67 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Resistencia a la tracción | 23.0 °C | 42 MPa Show Supplier Material materials with Resistencia a la tracción of 42 MPa | ASTM D 638 | yld, Type I, 50 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 389 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 389 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 7.38E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7.38E-5 1/K | ASTM E 831 | -40°C to 95°C | ||
Heat deflection temperature, 0.45 MPa | 93 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 93 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 82 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 82 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Temperatura de flexión bajo carga | 82 - 93 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 82 - 93 °C | ||||
Inflamabilidad | UL Recognized, 94V-1 Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥3mm UL 94 <br> Radiant Panel Listing: TRUE- UL Tested <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221153- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 60Hz | 23.0 °C | 2.8 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.8 [-] | ASTM D 150 | 50/60 Hz |
Dissipation factor, 1MHz | 23.0 °C | 3.5E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 3.5E-3 [-] | IEC 60250 |
Dissipation factor, 50Hz | 23.0 °C | 4E-3 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 4E-3 [-] | ASTM D 150 | 50/60 Hz |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 2 |
Rigidez dieléctrica | 23.0 °C | 24.8 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 24.8 kV/mm | ASTM D 149 | in oil, 3.2 mm |
Índice de seguimiento comparativo | 23.0 °C | 2 V Show Supplier Material materials with Índice de seguimiento comparativo of 2 V | UL 746A | (UL) {PLC} |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Data Transfer, Rail Cabin Interiors, Rail Seating, Wiring Devices, Wireless Communications | |
Availability | Americas | |
Processing methods | Drying Time (Cumulative): 8hrs | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |