General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad relativa | 23.0 °C | 1.09 [-] Show Supplier Material materials with Densidad relativa of 1.09 [-] | ASTM D 792 | |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 83 % Show Supplier Material materials with Elongación of 83 % | ASTM D 638 | brk, Type I, 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 336 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 336 J/m | ASTM D 256 |
Instrumented Impact, at Peak | 23.0 °C | 31 J Show Supplier Material materials with Instrumented Impact, at Peak of 31 J | ASTM D 3763 | 23°C |
Módulo de flexión | 23.0 °C | 2.3 GPa Show Supplier Material materials with Módulo de flexión of 2.3 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Resistencia a la flexión | 23.0 °C | 95 MPa Show Supplier Material materials with Resistencia a la flexión of 95 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Resistencia a la tracción | 23.0 °C | 62 MPa Show Supplier Material materials with Resistencia a la tracción of 62 MPa | ASTM D 638 | yld, Type I, 50 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 336 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 336 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 179 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 179 °C | ASTM D 648 | 6.4 mm, unannealed | |
Temperatura de flexión bajo carga | 179 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 179 °C | ||
Inflamabilidad | UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=220758- - |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 1.3 % Show Supplier Material materials with Contracción of 1.3 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Exterior, Heavy Vehicles | |
Availability | Americas | |
Processing methods | Barrel - Zone 1 Temperature: 270 to 280.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |