General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad relativa | 23.0 °C | 1.27 [-] Show Supplier Material materials with Densidad relativa of 1.27 [-] | ASTM D 792 | |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 1.6 % Show Supplier Material materials with Elongación of 1.6 % | Modified ASTM D638 | 5mm/min |
Resistencia a la flexión | 23.0 °C | 66 MPa Show Supplier Material materials with Resistencia a la flexión of 66 MPa | Modified ASTM D790 | 5mm/min |
Resistencia a la tracción | 23.0 °C | 124 MPa Show Supplier Material materials with Resistencia a la tracción of 124 MPa | Modified ASTM D638 | 5mm/min |
Aplicaciones térmicas
Technological properties
Property | ||
---|---|---|
Application areas | PANELS FOR AUTOMOBILES | |
Availability | Americas | |
Processing methods | Extruder L/D: 24- | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |