Description

30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.

Los datos sobre este material han sido proporcionados por Sabic.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValueComment

Absorción de agua

23.0 °C

0.9 %

Show Supplier Material materials with Absorción de agua of 0.9 %

ISO 62-1 | (23°C/saturated)

Densidad

23.0 °C

1.48 g/cm³

Show Supplier Material materials with Densidad of 1.48 g/cm³

ISO 1183

Densidad relativa

23.0 °C

1.48 [-]

Show Supplier Material materials with Densidad relativa of 1.48 [-]

ASTM D 792 |

Moisture absorption

23.0 °C

0.5 %

Show Supplier Material materials with Moisture absorption of 0.5 %

ISO 62 | (23°C / 50% RH)

Mecánica

PropertyTemperatureValueComment

Elongación

23.0 °C

2 %

Show Supplier Material materials with Elongación of 2 %

ISO 527 | break, 5 mm/min

Impact strength, Izod notched, ASTM

23.0 °C

39 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 39 J/m

ASTM D 256

Impact strength, Izod unnotched, ASTM

23.0 °C

330 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 330 J/m

ASTM D 4812 | 23°C

Instrumented Impact, Total Energy

23.0 °C

15 J

Show Supplier Material materials with Instrumented Impact, Total Energy of 15 J

ASTM D 3763 | 23°C

Módulo de flexión

23.0 °C

5.5 GPa

Show Supplier Material materials with Módulo de flexión of 5.5 GPa

ISO 178 | 2 mm/min

Módulo elástico

23.0 °C

5.3 GPa

Show Supplier Material materials with Módulo elástico of 5.3 GPa

ISO 527 | 1 mm/min

Resistencia a la flexión

23.0 °C

145 MPa

Show Supplier Material materials with Resistencia a la flexión of 145 MPa

ISO 178 | yield, 2 mm/min

Resistencia a la tracción

23.0 °C

80 MPa

Show Supplier Material materials with Resistencia a la tracción of 80 MPa

ISO 527 | yield, 5 mm/min

Resistencia al choque, ensayo Charpy entallado

23.0 °C

4 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4 kJ/m²

ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, -30°C

Resistencia al choque, ensayo Charpy no entallado

23.0 °C

25 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 25 kJ/m²

ISO 179/1eU | Unnotch Edgew 80*10*4 sp=62mm, -30°C

Resistencia al choque, ensayo Izod entallado

23.0 °C

5 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 5 kJ/m²

ISO 180/1A | 80*10*4, 23°C

Resistencia al choque, ensayo Izod no entallado

23.0 °C

25 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 25 kJ/m²

ISO 180/1U | 80*10*4, 23°C

Aplicaciones térmicas

PropertyTemperatureValueComment

Ball Pressure Test

Passes

IEC 60695-10-2 | 125°C +/- 2°C

Coeficiente de dilatación térmica

23.0 °C

3.2E-5 1/K

Show Supplier Material materials with Coeficiente de dilatación térmica of 3.2E-5 1/K

ISO 11359-2 | 23°C to 150°C

Coeficiente de dilatación térmica transversal

23.0 °C

3.5E-5 1/K

Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 3.5E-5 1/K

ISO 11359-2 | 23°C to 150°C

Conductividad térmica

23.0 °C

0.32 W/(m·K)

Show Supplier Material materials with Conductividad térmica of 0.32 W/(m·K)

ISO 8302

Heat deflection temperature, 0.45 MPa

204 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 204 °C

ISO 75/Bf | Flatw 80*10*4 sp=64mm

Heat deflection temperature, 1.80 MPa

192 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 192 °C

ISO 75/Af | Flatw 80*10*4 sp=64mm

Relative temperature index, electrical

105 °C

Show Supplier Material materials with Relative temperature index, electrical of 105 °C

UL 746B

Relative temperature index, mechanical impact

105 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C

UL 746B

Relative temperature index, mechanical strength

105 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 105 °C

UL 746B

Temperatura de flexión bajo carga

192 - 204 °C

Show Supplier Material materials with Temperatura de flexión bajo carga of 192 - 204 °C

Temperatura de reblandecimiento Vicat

213 °C

Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 213 °C

ISO 306 | Rate B/120

Inflamabilidad

UL Recognized, 94V-0 Flame Class Rating: ≥0.4mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221101- -

Eléctrico

PropertyTemperatureValueComment

High Amp Arc Ignition

23.0 °C

0.4 mm

Show Supplier Material materials with High Amp Arc Ignition of 0.4 mm

≥, UL 746A | PLC 4

High Volt Arc Track Rate

23.0 °C

4 PLC Code

Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code

UL 746A | (PLC)

Hot-Wire Ignition

23.0 °C

3 mm

Show Supplier Material materials with Hot-Wire Ignition of 3 mm

≥, UL 746A | PLC 1

Índice de seguimiento comparativo

23.0 °C

4 V

Show Supplier Material materials with Índice de seguimiento comparativo of 4 V

UL 746A | (UL) {PLC}

Rheological Properties

PropertyTemperatureValueComment

Contracción

23.0 °C

0.4 %

Show Supplier Material materials with Contracción of 0.4 %

SABIC method | 3.2 mm

Contracción transversal

23.0 °C

0.4 %

Show Supplier Material materials with Contracción transversal of 0.4 %

SABIC method | 3.2 mm

Velocidad de flujo de la masa derretida

13.7 g/10min

Show Supplier Material materials with Velocidad de flujo de la masa derretida of 13.7 g/10min

ASTM D 1238 | 337°C/6.6 kgf

Velocidad de flujo del volumen derretido

14 cm³/10min

Show Supplier Material materials with Velocidad de flujo del volumen derretido of 14 cm³/10min

ISO 1133 | MVR at 360°C/5.0 kg

Technological properties

Property
Application areas

Wiring Devices

Availability

Europe,Asia,Americas

Processing methods

Back Pressure: 0.3 to 0.7MPa
Nozzle Temperature: 345 to 400.0°C
Maximum Moisture Content: 0.02%
Screw Speed: 40 to 70.0rpm
Mold Temperature: 135 to 165.0°C
Drying Time: 4 to 6.0hrs
Shot to Cylinder Size: 40 to 60.0%
Middle - Zone 2 Temperature: 340 to 400.0°C
Vent Depth: 0.025 to 0.076mm
Rear - Zone 1 Temperature: 330 to 400.0°C
Drying Temperature: 150°C
Drying Time (Cumulative): 24hrs
Front - Zone 3 Temperature: 345 to 400.0°C
Melt Temperature: 350 to 400.0°C

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.